II-electrode ye-E2594-16imele ukusetshenziswa kokushisela okusezingeni eliphezulu okwenzelwe izinhlelo zokusebenza ezibalulekile ezidinga amandla akhethekile kanye nokumelana nokugqwala. Le electrode, evumelana nesigaba se-AWS E2594-16, iwumkhiqizo wokushisela wensimbi ovikelwe (i-SMAW). Yakhiwe ngokucophelela ukuze ifake insimbi yokushisela yensimbi engagqwali ephindwe kabili ehlanganisa izakhiwo ezincane ze-austenitic kanye ne-ferritic, okuholela ekuhlanganiseni okuqinile nokuthembekile kwezindawo zezimboni ezidinga amandla.
Le electrode ethize ye-E2594-16 ibonakaliswa okuqukethwe kwayo okuphansi kakhulu kwekhabhoni ne-nitrogen kanye nokwengezwa kwe-titanium, okufakwe ngaphakathi kwengubo esuselwe ku-lime (calcium). Ingubo inikeza i-arc ezinzile, ukuchitheka okuncane, kanye nokususwa kwe-slag okulula, okuthuthukisa kakhulu ukushibilika kanye nokusebenza kahle komqhubi. Ukwakheka kwentambo eyinhloko kanye nengubo kusebenza ndawonye ukukhiqiza insimbi yokushibilika ehlangabezana nezidingo zamakhemikhali eziqinile ze-AWS A5.4/A5.4M specification.
Isicelo esiyinhloko se-I-Electrode ye-E2594-16Itholakala ekushiseleni izinsimbi ezingagqwali ezimbili, ezivame ukubonwa yi-UNS S32750 kanye namazinga afanayo. Ifaneleka kahle kakhulu ezintweni ezidalulwe ezindabeni ezigqwalisayo ezinamandla, njengalezo ezitholakala ogwini lolwandle, ekucubungulweni kwamakhemikhali, ku-oyili negesi, kanye nasezimbonini ze-petrochemical. Ukushisela okuphumela kukho kubonisa ukumelana okuhle kakhulu nokuqhekeka kwemigodi, ukugqwala kwemifantu, kanye nokuqhekeka kokugqwala kokucindezeleka, okuqinisekisa ubuqotho besikhathi eside besakhiwo esishiselwe.
Izakhiwo zemishini zensimbi yokushisela ezifakwe yi-E2594-16 Electrode ziphakeme kakhulu. Abasebenzisi bangalindela amandla aphezulu okushisela kanye nokuqina okuhle, okubalulekile ezingxenyeni ezisebenza ngaphansi kokucindezeleka okuphezulu nasezindaweni eziphansi kwezinga lokushisa. Isakhiwo esincane esilinganiselwe esitholakala ngezinqubo ezifanele zokushisela siyisihluthulelo sokuthola lezi zakhiwo zemishini ezifanele kanye nezici zokusebenza.
II-Electrode ye-E2594-16iwumshini wokushisela wekhwalithi ephezulu osetshenziswayo onikeza abakhiqizi ikhambi elithembekile lokuhlanganisa izinsimbi ezingagqwali ezimbili. Ukwakheka kwayo okulawulwayo kanye nokugqoka kwekhwalithi ephezulu kuqinisekisa imiphumela ehambisanayo, okuhlangabezana nezidingo ezibalulekile zemboni yanamuhla. Le electrode imele njengethuluzi eliyisisekelo lokuqinisekisa ukuqina nokuphepha kwezakhiwo ezishisiwe ezisetshenziswayo ezigqwalisayo nezinamandla aphezulu.
Isikhathi sokuthunyelwe: Septhemba-23-2025