I-AF2594-16 (AWS E2594-16) iyi-electrode yensimbi engenasici ene-ultra-low carbon nitrogen ene-duplex ene-titanium-calcium coating.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Stainless Steel WeldingI-Electrode

AF2594-16

I-AWS A5.4 E2594-16

Incazelo: I-AF2594-16 iyi-electrode yensimbi engenasici ene-ultra-low carbon nitrogen ene-duplex ene-titanium-calcium coating.Ingasetshenziselwa kokubili i-AC ne-DC.I-PRE (i-pitting resistance value elinganayo noma inkomba ye-pitting) ≥ 40, insimbi efakiwe inokumelana okuhle kokuqhekeka okushisayo.Ngenxa yokuqukethwe kwekhabhoni ephansi kanye nenani elithile le-molybdenum ne-nitrogen, insimbi efakiwe inokumelana kahle nokugqwala komgodi kanye nokuqhekeka kokugqwala kwengcindezi.

Isicelo: Isetshenziselwa kakhulu ukushisela uhlobo olufanayo lwensimbi engagqwali eyi-duplex kuwoyela wasolwandle, igesi yemvelo kanye nezimboni ze-petrochemical, njenge-00Cr25Ni7Mo4N, njll.

 

Ukwakheka kwamakhemikhali ensimbi ye-weld(%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤1.00

24.0 ~ 27.0

8.0 ~ 10.5

3.5 ~ 4.5

0.20 ~ 0.30

≤0.75

≤0.030

≤0.040

 

 

Izici zemishini ye-weld metal:

Into yokuhlola

Amandla aqinile

Mpa

Ukwelula

%

Kuqinisekisiwe

≥760

≥15

 

Okwamanje okunconyiwe:

Ububanzi benduku

(mm)

2.5

3.2

4.0

5.0

I-Welding Yamanje

(A)

50 ~ 80

80 ~ 120

120 ~ 150

150 ~ 200

 

Isaziso:

1. I-electrode kufanele ibhakwe ihora elingu-1 endaweni engaba ngu-250 ℃ ngaphambi kokusebenza kokushisela;

2. Kubalulekile ukuhlanza okugqwalile, isikali sikawoyela, amanzi, nokungcola ezingxenyeni zokushisela ngaphambi kokushisela.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Siye sahlanganyela ekukhiqizenii-electrode ye-weldings, izinduku zokushisela, futhiizinto ezisetshenziswayo zokushiselaiminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ihlanganisa ama-electrode ensimbi engagqwali, ama-electrode welding steel, i-low alloy welding electrode, ama-electrode welding angaphezulu, ama-electrode welding we-nickel & cobalt alloy, izintambo zokushisela zensimbi emnene & ne-alloy ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe igesi eziguquguqukayo, izintambo zokushisela i-aluminium, i-arc welding engaphansi kwamanzi.izintambo, izintambo zokushisela i-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode ama-tungsten, ama-electrode okugobhoza ikhabhoni, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 


  • Okwedlule:
  • Olandelayo: