E316HT1-1 Insimbi engagqwali flux cored wire

Incazelo emfushane:

Inokusebenza okuhle kakhulu kwenqubo yokushisela njenge-arc ezinzile, i-spatter encane, ukususwa kwe-slag okuhle, ukondla ngocingo okuzinzile, nokuma okuhle.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

E316HT1-1 Insimbi engagqwali flux cored wire

Incazelo Yomkhiqizo
Ihambisana nezinga: GB/T17853 E316T1-1
I-AWS A5.22 E316HT1-1

Izici kanye nokusetshenziswa
1. Ngenxa yokuthi iqukethe inani elithile lekhabhoni, ifanele ukushisela imishini yensimbi engagqwali ekwazi ukumelana nokushisa okuphezulu;
2. Inokusebenza okuhle kakhulu kwenqubo yokushisela njenge-arc ezinzile, i-spatter encane, ukususwa kwe-slag okuhle, ukuphakelwa kocingo okuzinzile, nokuma okuhle;
3. Ngenxa yokuqukethwe okuphezulu kwe-Mo, ukumelana nokugqwala kunamandla;
4. Ifanele i-18%Cr-12%Ni-2%Mo welding ku-petrochemical, isitsha sokucindezela, imishini yezokwelapha nokudla, umanyolo nezinye izimboni.

Ukwakheka kwamakhemikhali (wt%)

Ingxubevange wt% C Mn Futhi Cr In Mo P S Nge
I-GB/T 0.08 0.5-2.5 1.0 17.0-22.0 11.0-14.0 2.0-3.0 0.040 0.030 0.50
AWS 0.04-0.08 0.5-2.5 1.0 17.0-22.0 11.0-14.0 2.0-3.0 0.040 0.030 0.75
Inani lesibonelo 0.50 1.45 0.50 18.05 12.00 2.35 0.020 0.005 0.05

 
Ukuziphatha kwemishini

Ukuziphatha kwemishini Isivuno samandla e-MPa Amandla e-MPa aqinile Elongation% Inani lomthelela J/℃
I-GB/T - 520 30 -
AWS - 520 30 -
Inani lesibonelo - 560 35 -

 
Ibanga lamanje elinconyiwe: (DC+)

Ububanzi bentambo yokushisela (mm) 1.2 1.6
Amandla kagesi (V) 22-36 26-38
Okwamanje (A) 120-260 200-300
Ubude bomile (mm) 15-20 18-25
Ukugeleza kwegesi (l/min) 15-25 15-25

 
Izinyathelo Zokushisela
1. Sebenzisa igesi evikelayo ye-CO2 enobumsulwa obungu-≥99.98% kanye nokugeleza kwegesi okungu-20-25L/min.
2. Izinga lokushisa eliphakathi kwesiteshi: 16~100 ℃.
3. Uma u-welding, kuyadingeka ukuvikela emoyeni ukuvimbela ukukhubazeka kwe-welding ekuhlakazweni kwegesi evikelayo.Amafutha, amanzi, njll. endaweni yokushisela kufanele kukhishwe.
4. Sebenzisa intambo yokushisela ngokushesha ngangokunokwenzeka ngemva kokuvula iphakheji.Uma ingasetshenziswanga, thatha izinyathelo zokuvikela umswakama.

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besizibandakanya ekukhiqizeni ama-electrode wokushiselaizinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ihlanganisa ama-electrode ensimbi engagqwali, ama-electrode welding steel, i-low alloy welding electrode, ama-electrode welding angaphezulu, ama-electrode welding we-nickel & cobalt alloy, izintambo zokushisela zensimbi emnene & ne-alloy ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe igesi eziguquguqukayo, izintambo zokushisela i-aluminium, i-arc welding engaphansi kwamanzi.izintambo, izintambo zokushisela i-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode ama-tungsten, ama-electrode okugobhoza ikhabhoni, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.


  • Okwedlule:
  • Olandelayo: