Intambo Yokushisela Yensimbi Engagqwali Ene-Flux Cored Wire E309LT-1 Flux-cored Wire

Incazelo emfushane:

I-E309LT-1 isetshenziswa kakhulu ezisekelweni zensimbi zokwakheka okufanayo njenge-AISI Types 301, 302, 304, 305 kanye ne-308. Okuqukethwe kwekhabhoni okuphezulu okungu-0.04% kuvumela ukumelana okukhulu nokugqwala kwe-intergranular futhi kunciphisa nemvula ye-carbide.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Insimbi engagqwaliI-Flux CoredIntambo E309LT-1

ISINGENISO
I-E309LT-1 ivame ukusetshenziswa kakhulu kwizinsimbi eziyisisekelo zokwakheka okufanayo njenge-AISI Types 301, 302, 304, 305 kanye ne-308. Okuqukethwe kwekhabhoni okuphezulu okungu-0.04% kuvumela ukumelana okukhulu nokugqwala kwe-intergranular futhi kunciphisa imvula ye-carbide. Lezi zintambo zenzelwe ukusetshenziswa nge-CO2 engu-100% noma i-80% Ar/20% CO2 shielding gas. Amandla okusebenza phezu kwezilungiselelo eziningi zamanje avumela amazinga okufakwa acishe abe ngaphezu kuka-4 kunama-electrode amboziwe futhi afike ku-50% amakhulu kune-solid MIG wire. Nakuba izindleko ngepawundi yezintambo ze-Stainless Steel Flux-Cored zingase zibe ngaphezu kwezama-electrode amboziwe noma i-solid MIG wire, izindleko zakho ngepawundi yensimbi ye-weld efakwe ziyancipha kakhulu ngenxa yokusebenza kahle kokufakwa kanye nezindleko zokusebenza eziphansi. I-sheath yangempela yensimbi ye-stainless esetshenziswa ekukhiqizeni i-Aufhauser Flux-Cored Stainless iyisiqinisekiso sakho sokusebenza okubushelelezi, ama-weld ekhwalithi ye-x-ray kanye nokubukeka okuhle kwensimbi ye-stainless bead. I-Spatter iphansi kakhulu futhi i-slag iyazikhukhula yona.

IZICELO
Ukushisela ama-alloy afanayo ngezindlela ezibunjiwe noma ezibunjiwe
Ukushisela izinsimbi ezingafani, njengokuthi: ukuhlanganisa uhlobo 304 nensimbi ethambile, ukushisela uhlangothi lwensimbi engagqwali lwezinsimbi ezimbozwe uhlobo 304, nokusebenzisa ulwelwesi lweshidi lensimbi engagqwali kumashidi ensimbi yekhabhoni
Ngezinye izikhathi kusetshenziselwa ukushisela izinsimbi eziyisisekelo zohlobo lwe-304 ezimweni zokugqwala okukhulu
Isetshenziselwa ukumbozwa kwensimbi yekhabhoni uma kungadingeki ukwengezwa kwe-columbium.

ULWAZI OLUVAMILE
Ukwakheka Kwamakhemikhali

Ikhabhoni I-Chromium I-Nickel I-Molybdenum I-Manganese I-Silicon I-Phosphorus I-Sulphur Ithusi Insimbi
0.04 22.0-25.0 12.0-14.0 0.5 0.5-2.5 1.0 0.04 0.03 0.5 I-Rem

IZIMPAHLA EZIPHILAYO NEZEMIKHANIKA

Amandla Okudonsa 75,000 psi
Ubuningi –
Ukwelulwa, ubuncane % 30

 

IZIMISO ZIYAHLANGABEZA NOMA ZIYADLULA
I-AWS: A5.22
I-ASME: SFA 5.22

 

OSAYIZI ABAJWAYELEKILE NAMADAMETHA
Ububanzi: 0.035″, 0.045″, kanye no-1/16″

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besilokhu sihilelekile ekukhiqizeni ama-electrode okushisela,izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.