I-Nickel Alloy Welding Wire ERNiCrMo-3 Mig Welding Wire

Incazelo emfushane:

I-ERNiCrMo-3 iwucingo oluphezulu lwe-nickel alloy olwakhelwe ukushisela nokuhlanganisa ama-alloys asekelwe ku-nickel afana nama-625 noma izinto ezifanayo.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Nickel AlloyWelding WireI-ERNiCrMo-3

 

Amazinga

I-EN ISO 18274 – Ni 6625 – NiCr22Mo9Nb

I-AWS A5.14 – ER NiCrMo-3

 

Izici kanye nezicelo

Phezului-nickeli-alloy wire eyenzelwe ukushisela nokuhlanganisai-nickelama-alloys asekelwe njengama-625 noma izinto ezifanayo.

Okuqinile kudwetshwe ngendlela ekhetheke kakhulu ukuthola amashisela ahlanzekile nasezingeni eliphezulu anomthungo ogqamile kanye ne-ductility enhle kakhulu.

Insimbi yokushisela inezakhiwo ezinhle kakhulu zemishini emazingeni okushisa aphezulu naphansi.

Ukumelana kahle ne-pitting kanye nokugqwala kwengcindezi.

Izinga lokushisa elinconywayo lokusebenza lisukela ku-cryogenic ukuya ku-540°C.

Inxeba lesendlalelo esinembayo lezimpawu zokuphakela ngocingo eziphezulu.

Ivamise ukusetshenziswa embonini yezinqubo zamakhemikhali, ubunjiniyela basolwandle, izingxenye ze-nuclear reactor, i-aerospace nangaphakathi kwemishini yokulawula ukungcoliswa kwemvelo njll.

 

Izinto Eziyisisekelo Ezijwayelekile

I-Inconel 601, i-Incoloy 800, i-Alloy 625, i-Alloy 825, i-Alloy 926* * Uhlu olubonisayo, olungaphelele

 

Ukwakheka Kwekhemikhali %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

ubuningi

ubuningi

ubuningi

ubuningi

ubuningi

ubuningi

ubuningi

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

ubuningi

ubuningi

ubuningi

20.00

3.15

8.00

Okuncane

1.0

0.40

0.40

23.00

4.15

10.00

 

Izakhiwo Zemishini

Amandla Okuqina

≥760 MPa

Isivuno Amandla

≥415 MPa

Ukwelula

≥35%

Amandla Omthelela

≥100 J

Izakhiwo zikamshini ziyalinganiselwa futhi zingahluka kuye ngokushisa, igesi evikelayo, imingcele yokushisela nezinye izici.

Ukuvikela Amagesi

I-TS EN ISO 14175 - I1, I3

Izikhundla zokushisela

I-TS EN ISO 6947 PA, PB, PC, PD, PE, PF

Idatha yokupakisha

Ububanzi

Isisindo

Spool

I-Pallet Qty

1.00 mm

1.20 mm

15 Kg

15 Kg

BS300

BS300

72

72

Isikweletu:Nakuba yenziwe yonke imizamo yokuqinisekisa ukunemba kolwazi oluqukethwe, lolu lwazi lungase lushintshe ngaphandle kwesaziso futhi lungabhekwa kuphela njengolufanele ukuqondiswa okuvamile.