I-Nickel Alloy Welding Wire ERNiCrMo-3 Tig Wire

Incazelo emfushane:

I-ERNiCrMo-3 iwucingo oluphezulu lwe-nickel alloy olwakhelwe ukushisela nokuhlanganisa ama-alloys asekelwe ku-nickel afana nama-625 noma izinto ezifanayo.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Nickel AlloyWelding WireI-Tig WireI-ERNiCrMo-3

 

Izici kanye nezicelo

Phezului-nickeli-alloy wire eyenzelwe ukushisela nokuhlanganisai-nickelama-alloys asekelwe njengama-625 noma izinto ezifanayo.

Okuqinile kudwetshwe ngendlela ekhetheke kakhulu ukuthola amashisela ahlanzekile nasezingeni eliphezulu anomthungo ogqamile kanye ne-ductility enhle kakhulu.

Insimbi yokushisela inezakhiwo ezinhle kakhulu zemishini emazingeni okushisa aphezulu naphansi.

Ukumelana kahle ne-pitting kanye nokugqwala kwengcindezi.

Izinga lokushisa elinconywayo lokusebenza lisukela ku-cryogenic ukuya ku-540°C.

Ivamise ukusetshenziswa embonini yezinqubo zamakhemikhali, ubunjiniyela basolwandle, izingxenye ze-nuclear reactor, i-aerospace nangaphakathi kwemishini yokulawula ukungcoliswa kwemvelo njll.

Izinto Eziyisisekelo Ezijwayelekile

Inconel 601, Incoloy 800, Ingxubevange 625, Ingxubevange 825, Ingxubevange 926*
* Uhlu olunemifanekiso, hhayi oluphelele

 

Amazinga
I-EN ISO 18274 – Ni 6625 – NiCr22Mo9Nb
I-AWS A5.14 – ER NiCrMo-3

 

Ukwakheka Kwekhemikhali %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

ubuningi

ubuningi

ubuningi

ubuningi

ubuningi

ubuningi

ubuningi

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

ubuningi

ubuningi

ubuningi

20.00

3.15

8.00

imiz

1.0

0.40

0.40

23.00

4.15

10.00

 

Izakhiwo Zemishini
Amandla Okuqina ≥760 MPa  
Isivuno Amandla ≥415 MPa  
Ukwelula ≥35%  
Amandla Omthelela ≥100 J  

Izakhiwo zikamshini ziyalinganiselwa futhi zingahluka kuye ngokushisa, igesi evikelayo, imingcele yokushisela nezinye izici.

 

Ukuvikela Amagesi

I-TS EN ISO 14175 TIG: I1 (Argon)

 

Izikhundla zokushisela

I-TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Idatha yokupakisha
Ububanzi Ubude Isisindo  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 

 

Isibopho sezomthetho: Nakuba yenziwe yonke imizamo yokuqinisekisa ukunemba kolwazi oluqukethwe, lolu lwazi lungashintsha ngaphandle kwesaziso futhi lungabhekwa kuphela njengolufanele ukuqondiswa okuvamile.

 


  • Okwedlule:
  • Olandelayo: