I-Nickel Alloy Welding Wire ERNi-1 I-Nickel Tig Wire Filler Metal

Incazelo emfushane:

I-ER-Ni1 isetshenziselwa ukushisela nokugqoka ama-alloys e-Nickel 200 kanye ne-Nickel 201.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Nickel AlloyWelding WireI-Tig WireI-ERNi-1

Amazinga
EN ISO 18274 – Ni 2061 – NiTi3
I-AWS A5.14 – ER Ni-1

 

Izici kanye nezicelo

I-ER-Ni1 isetshenziselwa ukushisela nokugqoka ama-alloys e-Nickel 200 kanye ne-Nickel 201.

Ilungele ukuhlanganisa ama-Monel alloys kanye ne-copper-i-nickelama-alloys kuya ku-carbon steels.

I-Ni1 iqukethe i-titanium eyanele yokulawula i-weld-metal porosity ezinqubweni zokushisela.

Ivamise ukusetshenziswa ezimbonini zokucubungula amakhemikhali, ukukhiqizwa kwefayibha yokwenziwa kanye nemishini yokucubungula ukudla njll.

 

Izinto Eziyisisekelo Ezijwayelekile

I-Nickel 200 kanye ne-201*
* Uhlu olunemifanekiso, hhayi oluphelele

 

Ukwakheka Kwekhemikhali %
C% Mn% Fe% P% S% Si%  
ubuningi ubuningi ubuningi ubuningi ubuningi ubuningi  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Cu% Ni% Co% Ti% Al%    
ubuningi 93.00 ubuningi 2.00 ubuningi    
0.20 imiz 1.00 3.50 1.00    

 

Izakhiwo Zemishini
Amandla Okuqina ≥410 MPa  
Isivuno Amandla ≥200 MPa  
Ukwelula ≥30 %  
Amandla Omthelela ≥100 J  

Izakhiwo zikamshini ziyalinganiselwa futhi zingahluka kuye ngokushisa, igesi evikelayo, imingcele yokushisela nezinye izici.

 

Ukuvikela Amagesi

I-TS EN ISO 14175 TIG: I1 (Argon)

 

Izikhundla zokushisela

I-TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Idatha yokupakisha
Ububanzi Ubude Isisindo  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 Kg

5 Kg

 

 

Isibopho sezomthetho: Nakuba yenziwe yonke imizamo yokuqinisekisa ukunemba kolwazi oluqukethwe, lolu lwazi lungashintsha ngaphandle kwesaziso futhi lungabhekwa kuphela njengolufanele ukuqondiswa okuvamile.