I-ERCUAL-A1 Aluminium Bronze Welding Wire, Aluminium Tig Rod, Aluminium Mig Welding

Incazelo emfushane:

I-ERCuAl-A1 Aluminium Bronze Welding Wire iyingxube ye-iron-free, i-aluminium yethusi etholakala ngocingo olugobile kanye nenduku yensimbi engu-36” bare-filler ukuze isetshenziswe nezinqubo zokushisela ze-gas metal-arc kanye ne-gas tungsten-arc ngokulandelana.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-ERCuAl-A1 Aluminium Bronze Welding Wire iyingxube ye-iron-free, i-aluminium yethusi etholakala ngocingo olugobile kanye nenduku yensimbi engu-36” bare-filler ukuze isetshenziswe nezinqubo zokushisela ze-gas metal-arc kanye ne-gas tungsten-arc ngokulandelana.

Amadiphozi e-ERCuAl-A1 Aluminium Bronze Welding Wire asetshenziswa ngokuyinhloko ukuze amboze izindawo ezithwalayo nezingagugi ezidinga ubulukhuni obucishe bube ngu-125 BHN nokumelana nokugqwala ikakhulukazi emanzini anosawoti, usawoti wensimbi, nama-asidi amaningi asetshenziswa ngokuvamile ekugxilweni okuhlukahlukene namazinga okushisa.Le alloy ayinconyelwe ukujoyina ngoba idiphozi ayinakho ukuthambekela kokushisa okuncane.

Izicelo ze-ERCuAl-A1 Aluminium Bronze Welding Wire Aluminium Bronze Welding Wire zihlanganisa amashidi eshubhu, izihlalo zamavalvu, amahhuku okukhetha, ama-impeller, izitshalo zamakhemikhali, nezigayo ze-pulp.

I-ERCUAL-A1 ALUMINUM EBRONZE WELDING WIRE IZIMPAHLA ZOKUSETSHENZISWA KOMZIMBA KANYE NE-MACHHANICAL:

Okuqinile-Izinga lokushisa 1030 ℃
Ukuminyana 7.7kg/dm³
Ukwelula 40-45%
I-Liquids-Temperature 1040 ℃
Amandla Okuqina 380-450N/mm²
Ukuqina kweBrinell 100HB

I-ERCUAL-A1 ALUMINUM IBRONZE WELDING WIRE PING:

I-MIG Ububanzi 0.8 - 2.0mm Ukupakisha D100mm D200mm D300mm Isisindo 1kg/5kg/12.5kg/13.6kg/15kg
0.030″-5/64″ 2lb/10lb/27lb/30lb/33lb
I-TIG Ububanzi 1.6 - 6.4mm Ubude 457mm / 914mm Ukupakisha 5kg / ibhokisi 25kg / ibhokisi 10kg / iphakethe plastic
1/16″ - 1/4″ 18" / 36" 10lb / ibhokisi 50lb / ibhokisi 10kg / iphakethe plastic

Sicela uqaphele: Imikhiqizo ye-spools yamapulangwe engu-500lb iyatholakala uma icelwa.

I-ERCUAL-A1 ALUMINUM YEBRONZE WELDING WIRE COMPOSITE CHEMICAL COMPOSITE(%):

Okujwayelekile ISO24373 I-GB/T9460 I-GB/T9460 I-BS EN14640 AWS A5.7 I-DIN 1733
Ikilasi ku6100 I-SCu6100 I-SCu6100A ku6100 C61000 2.0921
Ingxubevange Kual7 Kual7 Kual8 Kual8 I-ERCuAl-A1 I-SG-CuAl8
Cu bal. bal. bal. bal. bal. bal.
Al 6.0-8.5 6.0-8.5 7.0-9.0 6.0-9.5 6.0-8.5 7.5-9.5
Fe - - ubuningi 0.5 0.5 - ubuningi 0.5
Mn 0.5 ubuningi 0.5 ubuningi 0.5 0.5 0.5 ubuningi 1.0
Ni - - ubuningi 0.5 0.8 - ubuningi 0.8
P - - - - - -
Pb 0.02 - ubuningi 0.02 0.02 0.02 ubuningi 0.02
Si 0.2 ubuningi 0.1 ubuningi 0.2 0.2 0.1 ubuningi 0.2
Sn - - ubuningi 0.1 - - -
Zn 0.2 ubuningi 0.2 ubuningi 0.2 0.2 0.2 ubuningi 0.2
okunye 0.4 ubuningi 0.5 ubuningi 0.2 0.4 0.5 ubuningi 0.4