I-ERNiFe-CI Nickel Alloy Welding Wire Tig Filler Rod Mig kanye neTig Welding Rods

Incazelo emfushane:

I-ERNiFe-CI isetshenziselwa ukushisela i-cast iron.Le nsimbi yokugcwalisa isetshenziswa kakhulu ukumboza ama-cast iron rolls.Ibuye isetshenziselwe ukulungisa ama-castings.Izinga lokushisa langaphambili kanye ne-interpass elingu-175ºC (350ºF) eliphansi liyanconywa ngesikhathi sokushisela, ngaphandle kwalokho izindawo ezithintekile zokushisela zingadala imifantu.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-ERNiFe-CI isetshenziselwa ukushisela i-cast iron.Le nsimbi yokugcwalisa isetshenziswa kakhulu ukumboza ama-cast iron rolls.Ibuye isetshenziselwe ukulungisa ama-castings.Izinga lokushisa langaphambili kanye ne-interpass elingu-175ºC (350ºF) eliphansi liyanconywa ngesikhathi sokushisela, ngaphandle kwalokho izindawo ezithintekile zokushisela zingadala imifantu.

I-Ni 55 (isigaba se-AWS asicacisiwe) intambo ye-Nickel ebizwa ngokuthi engu-55%.Okuqukethwe kwe-Nickel ephansi kwenza le ngxube yonge kakhulu kune-Ni 99. Amadiphozi e-Weld ngokuvamile akwazi ukusebenza ngomshini, kodwa ngaphansi kwezimo zokuxutshwa okuphezulu, ama-welds angaba nzima futhi kube nzima ukuwenza ngomshini.Ivame ukusetshenziselwa ukulungisa ama-castings anezingxenye ezinzima noma ezinzima.Njengoba kuqhathaniswa ne-Ni 99, ama-welds enziwe nge-55 Ni anamandla futhi ane-ductile, futhi abekezelela i-phosphorous ekubunjweni.Iphinde ibe ne-coefficient ephansi yokunwetshwa kune-Ni 99, okuholela ekuqhekekeni komugqa wokuhlanganisa okumbalwa.

UKWAKHIWA KWEKHEMICAL:

I-NickelNi45.0-60.0%

I-IronFebalance

I-SiliconSimax 4.0%

I-ManganeseMn2.5%

I-CopperCu2.5%

I-CarbonCmax 2.0%

I-AluminiumAlmax 1.0%

IZIMPILO ZOMKHETHI:

Amandla e-Tensile Rm (MPa) Amandla esivuno Rp0.2 (MPa) I-Elongation A %
imiz.393-579 (57-84 psi) 296-434 (40-64 psi) 6-13

AMAFOMU OMKHIQIZO:

Umkhiqizo

Ububanzi, mm

Ubude, mm

Intambo yokushisela i-MIG/GMAW

0.8, 1.0, 1.2, 1.6, 2.0, 2.4, 2.5, 3.2

-

Izinduku zokushisela i-TIG/GTAW

2.0, 2.5, 3.2, 4.0, 5.0

915 - 1000

Intambo yokushisela i-SAW

2.0, 2.4, 3.2, 4.0, 5.0

-

I-Electrode core wire

2.0, 2.5, 3.20, 3.25, 4.0, 5.0

250, 300, 350, 400, 450, 500

IZICELO:

I-Binary Nickel-Iron (Ni-Fe) kanye nama-alloys e-Ni based welding complex ahlinzekwa ngezinduku zokushisela nezintambo ezinobude obujwayelekile noma ubude kuze kufike esicelweni sabathengi.Ezimweni ezijwayelekile zesevisi, ukwakheka kwamakhemikhali kuyatholakala kokuqukethwe kwe-Ni okuhlukahlukene ngokuvumelana nezindinganiso eziningi zaseMelika nezaseYurophu.