Izinto Zokushisela Zensimbi Engagqwali ze-AWS A5.4 E310-16 Izinto Zokushisela Zensimbi Engagqwali

Incazelo emfushane:

I-A402 (AWS E310-16) iyi-electrode yensimbi engagqwali ye-austenitic ehlanzekile ye-Cr26Ni21 ene-titanium calcium coating.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Electrode Yokushisela Yensimbi Engagqwali

A402                                   

I-GB/T E310-16

I-AWS A5.4 E310-16

 Incazelo: I-A402 iyi-electrode yensimbi engagqwali ye-austenitic ehlanzekile ye-Cr26Ni21 ene-titanium calcium coating. Ingasetshenziswa kokubili i-AC ne-DC ngokusebenza okuhle kakhulu. Insimbi efakiwe inokumelana okuhle kwe-oxidation ngaphansi kwesimo sokushisa okuphezulu esingu-900 ~ 1100 ℃.

Ukusetshenziswa: Isetshenziselwa ukushisela uhlobo olufanayo lwensimbi engagqwali engamelana nokushisa olusebenza ngaphansi kwezimo zokushisa okuphezulu, futhi ingasetshenziswa futhi ekushiseleni izinsimbi ze-chromium eziqinile (njenge-Cr5Mo, i-Cr9Mo, i-Cr13 ne-Cr28, njll.) kanye nezinsimbi ezingafani.

 

 

Ukwakheka kwamakhemikhali kwensimbi eshidiwe (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

0.08 ~ 0.20

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

≤0.75

≤0.030

≤0.030

 

 

Izakhiwo zemishini zensimbi yokushisela:

Into yokuhlola

Amandla okudonsa

I-Mpa

Ukwelulwa

%

Kuqinisekisiwe

≥550

≥25

 

I-current enconyiwe:

Ububanzi benduku

(mm)

2.0

2.5

3.2

4.0

5.0

Ukushisela Kwamanje

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

 

Isaziso:

  1. I-electrode kumele ibhakwe ihora eli-1 cishe ku-250℃ ngaphambi kokusebenza kokushisela;
  2. Ngenxa yokuthi ukujula kokungena akujulile ngesikhathi sokushisela i-AC, ugesi we-DC kufanele usetshenziswe ngangokunokwenzeka ukuze kungene ngokujulile. Futhi ugesi akufanele ube mkhulu kakhulu ukuze kugwenywe ukubomvu kwenduku yokushisela.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 

 


  • Okwedlule:
  • Olandelayo: