I-A312 (AWS E309Mo-16) iyi-electrode yensimbi engagqwali ye-Cr23Ni13Mo2 ene-titanium calcium coating.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Ukushisela Insimbi EngagqwaliI-electrode

A312                                     

I-GB/T E309Mo-16

I-AWS A5.4 E309Mo-16

Incazelo: I-A312 iyi-electrode yensimbi engagqwali ye-Cr23Ni13Mo2 ene-titanium calcium coating. Ingasetshenziswa kokubili i-AC ne-DC ngokusebenza okuhle kakhulu. Inokumelana nokugqwala, ukuqhekeka, kanye nokushiswa kwe-oxidation okungcono kune-A302 ngoba insimbi efakiwe iqukethe i-molybdenum.

Ukusetshenziswa: Isetshenziselwa ukushisela uhlobo olufanayo lwesitsha sensimbi engagqwali esimelana nokugqwala yi-sulfuric acid medium (i-ammonia sulfide), futhi ingasetshenziswa futhi ekushiseleni ulwelwesi lwensimbi engagqwali, ipuleti lensimbi elimboziwe kanye nensimbi engafani.

 

Ukwakheka kwamakhemikhali kwensimbi eshidiwe (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Izakhiwo zemishini zensimbi yokushisela:

Into yokuhlola

Amandla okudonsa

I-Mpa

Ukwelulwa

%

Kuqinisekisiwe

≥550

≥25

 

I-current enconyiwe:

Ububanzi benduku

(mm)

2.0

2.5

3.2

4.0

5.0

Ukushisela Kwamanje

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

  1. I-electrode kumele ibhakwe ihora eli-1 cishe ku-150℃ ngaphambi kokusebenza kokushisela;
  2. Ngenxa yokuthi ukujula kokungena akujulile ngesikhathi sokushisela i-AC, ugesi we-DC kufanele usetshenziswe ngangokunokwenzeka ukuze kungene ukungena okujulile. Futhi ugesi akufanele ube mkhulu kakhulu ukuze kugwenywe ukubomvu kwenduku yokushisela.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besilokhu sihilelekile ekukhiqizeni ama-electrode okushisela,izinduku zokushisela, futhiizinto ezisetshenziswayo zokushiselaiminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 


  • Okwedlule:
  • Olandelayo: