EN 573-3: E AlSi12
I-DIN 1732: EL-Al Si12
EZIPHUMA NEZINTO ZOKWENZA:
Ukuze kufakwe i-arc welding, ama-aluminium axutshwe ngethusi, i-silicon, ne-magnesium.
Kuhle kakhulu futhi ekuhlanganiseni amazinga ahlukene e-aluminium.
I-electrode yokushisela i-arc ye-aluminium ye-silicon engu-12% ene-slag yokuziphakamisa ekhethekile. Amanye amazinga e-aluminium afana ne-Al 99, i-Al Mn, njll. nawo ayatholakala.
I-slag eyingqayizivele yokuziphakamisa.
Isembozo se-extruded flux esimhlophe esihlala isikhathi eside sidlula imikhiqizo evamile ekumelana nomswakama.
Kungenziwa ngemibala ehlukahlukene eyenziwe ngokwezifiso.
Itholakala kumathini okudonsa e-PURE ALUMINUM avaliwe angangenisi umoya noma ezikhwameni ze-foil ezipakishwe nge-vacuum ukuze ihlale isikhathi eside.
Itholakala futhi ngesimo se-TIG njengekhodi yento 6047, ngesimo se-MIG njengekhodi yento 7091 kanye nanjengento engenalutho.
I-ALLOY YOKUBIZA ISITOSHI NJENGEKHODI YENTO 2191:
| Ukuhlaziywa Kwensimbi Okuhlanganisiwe Konke (Isisindo Esijwayelekile %) | |||||
| Umbala we-Flux: Imibala Emhlophe noma Eyenziwe Ngokwezifiso | |||||
| 12.1 | .001 | .15 | .01 | .003 | .001 |
| Si | Cu | Fe | Mg | Mn | Zn |
| Ukushisela Kwamanje Nemiyalelo | ||
| I-Current Enconyiwe: I-DC Reverse (+) | ||
| Ububanzi (mm) | 3/32 (2.5) | 1/8 (3.25) |
| Isilinganiso Esincane Sokulinganisela | 50 | 70 |
| Isilinganiso Esiphezulu Somsindo | 80 | 120 |
Amasu Okushisela: Qala ngokusebenzisa ingxenye ephezulu yebanga le-amperage. Phakamisa i-electrode ngokushesha bese uhamba ngokushesha ugcine igebe le-arc eliseduze kakhulu.
Izikhundla Zokushisela: Ifulethi, Evundlile
AMAZINGA OKUBEKA ESIKHUNDLWENI:
| Ububanzi(mm) | Ubude (mm) | Insimbi Ehlanganisiwe/I-Electrode | Ama-electrode nge-lb (kg) ye-Weldmetal | Isikhathi Sokubekwa Kwe-Arc min/lb (kg) | Izilungiselelo ze-Amperage | Isilinganiso Sokubuyisela |
| 3/32 (2.5) | 14″ (350) | .14oz (4.3g) | 114 (251) | 110 (242) | 70 | 90% |
| 1/8 (3.25) | 14″ (350) | .23oz (6.5g) | 70 (153) | 62 (136) | 110 | 90% |
| 5/32 (4.0) | 14″ (350) | .33oz (9.6g) | 48 (107) | 47 (103) | 135 | 90% |
UKUPHAKISHA NOKULINGANISELA KWE-ELECTRODE OKULINGANISELEKILE:
| 3/32 (2.5) | 1/8 (3.25) | |
| Ubude (mm) | 14″ (350) | 14″ (350) |
| Ama-electrode / lb | 49 | 33 |
| Ama-electrode / kg | 108 | 73 |