Ukuhlukaniswa kwe-AWS: AWS 5.9
INCAZELO:
Intambo yokushisela yensimbi engagqwali inokusebenza kahle kakhulu kokumboza, ukusebenza kahle kobuchwepheshe bokushisela ekushiseleni okunezindawo zonke. Zisetshenziswa kabanzi embonini: isakhiwo sesakhiwo, izimoto, ubunjiniyela bebhuloho, imishini yezimayini, izitimela, ipayipi likawoyela, imishini ephethe umfutho wegesi, imishini kagesi, njll.
INOMBOLO YEMODELO NOSAYIZI:
1. Insizakalo ye-OEM yokunikezwa kwefektri.
2. Imodeli: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi njll.
3. Usayizi wentambo ye-MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. Usayizi wentambo ye-TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm .
ISINGENISO:
Sihlinzeka ngezinhlobo ezahlukene zocingo lokushisela lwensimbi engagqwali, okuhlanganisa ucingo lokushisela oluqinile lwe-Mig, ucingo lokushisela lwe-Tig rod kanye nocingo lokushisela olungaphansi kwe-arc, zonke zisezingeni eliphezulu futhi zithengiswa emhlabeni jikelele.
Ngaphandle kwe-308 ne-309, siphinde sinikeze i-304, 321, 347, 316L, 310, 2209, kanye ne-201. Kanye nemininingwane ekhethekile efana ne-318L, 904L, 2594, NiCrMo-3, Ni1.
UKUPHAKISHA:
Ukupakisha ucingo lokushisela i-Mig (iphakethe le-spool kanye ne-drum)
Ububanzi: 0.8 - 2.0mm
Iphakheji: 1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/drum, 200 kg/drum
Ukupakisha ucingo lokushisela induku ye-tig (ipayipi lepulasitiki)
Ububanzi: 1.0 - 5.0mm
Iphakheji: 5 kg/iphakethe
Ucingo lokushisela lwe-arc olucwiliswe emanzini
Ububanzi: 2.5 - 5.0mm
Iphakheji: 20kg/iphakethe, 25 kg/iphakethe
Ukupakisha okungathathi hlangothi kanye ne-OEM kwamukelekile!
IZINHLANGANO ZAMAKHEMIKI EZINTAMBO ZOKUSHINTSHA EZINGAKAGQI:
| Inombolo Yemodeli | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| I-ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| I-ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| I-ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| I-ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| I-ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| I-ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| I-ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| I-ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| I-ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| I-ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| I-ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| I-ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| I-ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| I-ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Inombolo Yemodeli | Amandla okudonsa i-Rm(Mpa) | Amandla okukhiqiza i-Rel noma i-Rp0.2(Mpa) | Ukwelulwa (%) | Inombolo Yemodeli | Amandla okudonsa i-Rm(Mpa) | Amandla okukhiqiza i-Rel noma i-Rp0.2(Mpa) | Ukwelulwa (%) |
| 304 | 550 | -- | 25 | I-ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | I-ER316 | 510 | 320 | 25 |
| I-ER307 | 590 | 350 | 25 | I-ER316L | 510 | 320 | 25 |
| I-ER308 | 550 | 350 | 25 | I-ER316LSi | 510 | 320 | 20 |
| I-ER308L | 510 | 320 | 25 | I-ER310 | 550 | 350 | 25 |
| I-ER308LSi | 510 | 320 | 25 | I-ER347 | 550 | 350 | 25 |
| I-ER309 | 550 | 350 | 25 | I-ER317 | 550 | 350 | 25 |
| I-ER309L | 510 | 320 | 25 | I-ER321 | 550 | 350 | 25 |
| Ukwakheka kwentambo yokushisela yensimbi engagqwali ye-TIG ne-MIG | ||||||||||
| YB5092-2005 | I-AWS | Ukwakheka Kwamakhemikhali % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | I-ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | I-ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | I-ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | I-ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | I-ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | I-ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | I-ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | I-ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | I-ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | I-ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | I-ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | I-ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | I-ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | I-ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | I-ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Inombolo 0.7 |
| H02Cr20Ni34Mo2Cu3Nb | I-ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Inombolo 0.35 |
| H08Cr20Ni10Ti | I-ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | I-Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | I-ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | I-Nb1xC-1.0 | |
| H12Cr26Ni21 | I-ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | I-ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | I-Cu 1.80 |
| H03Cr22Ni9Mo3N | I-ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | I-ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | I-ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | I-ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | I-ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | I-Cu;3 Nb;0.28 | |
| H08Cr26Ni5Mo2 | Ama-ER453 | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | I-ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.
Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.
I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.
Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.