Intambo Yokushisela ye-Arc Ecwiliswe ku-EM13K engu-2.5/3.2/4.0/5.0mm
Intambo yokushisela ye-arc ecmerged H10MnSi uhlobo lwentambo yokushisela yohlobo lwe-manganese kanye ne-silicon ephakathi.
1. Ihambisana ne-flux yokushisela yohlobo lwe-manganese oluphakathi nendawo kanye ne-silicon ephakathi nendawo.
2. Ayizweli ekugqwaleni kwensimbi eyisisekelo.
3. Inokwakheka okuhle kakhulu kobuhlalu kanye nokuhlukaniswa kwe-slag.
4. I-Monopole noma i-dipole. I-AC/DC.
5. Isetshenziselwa kokubili ukushisela ngesivinini esikhulu kanye nokushisela ngokugcwalisa ezintweni zensimbi zeklasi ezingama-50kg.
6. ukushisela enye insimbi yekhabhoni engu-501 Mpa kanye nensimbi ephansi ye-alloy
I-EM13K Ivumelana Nezinga Elijwayelekile: GB/T 5293 H10MnSi
I-AWS EM13K
I-ISO 14171-B-SU25
Imininingwane: Luhlobo lwentambo yokushisela enokuqukethwe okufanele kwe-manganese ne-silicon., Ihambisana ne-flux yokushisela yohlobo lwe-manganese oluphansi kanye nohlobo lwe-silicon oluphansi, Ayizweli ekugqwaleni kwensimbi eyisisekelo. Inokubumba okuhle kakhulu kobuhlalu, ikhono elihle kakhulu lokuhlukanisa i-slag.
Inhloso: Isetshenziswa nge-flux e-sintered LT.SJ101, ingasetshenziswa kokubili ekushiseni ngesivinini esikhulu ipuleti lensimbi elinamandla okunamathela angu-420N/mm2 kanye nasekushiseni kokugcwalisa. Isetshenziswa kabanzi ekushiseni ibhoyila, isitsha sokucindezela, ibhuloho, umkhumbi njll.
Ukwakheka Kwamakhemikhali (%)
| Ukwakheka Kwamakhemikhali | C | Mn | Si | S | P | Cr | Ni | Cu |
| Inani Lesiqinisekiso | ≤0.14 | 0.80~ 1.10 | 0.60~ 0.90 | ≤0.035 | ≤0.035 | ≤0.20 | ≤0.30 | ≤0.35 |
| Umphumela Ojwayelekile | 0.089 | 0.98 | 0.67 | 0.023 | 0.032 | 0.015 | 0.034 | 0.11 |
Izakhiwo Zemishini Zensimbi Egciniwe
| Into yokuhlola I-Flux | I-Rm(MPa) | I-ReL/Rp0.2(MPa) | A(%) | I-KV2(J) -20℃ |
| LT•SJ101 | 415~550 | ≥330 | ≥22 | ≥27 |
Usayizi Wezintambo Zokushisela
| Usayizi(mm) | Φ2.5 | Φ3.2 | Φ4.0 | Φ5.0
|