I-D132 (B-83) I-Electrode Yokushisela Eqinile, Induku Yokushisela Engaphezulu, Induku Yokushisela Ye-Arc

Incazelo emfushane:

I-electrode ye-hydrogen ephansi yokushisela kabusha. Ukushisela kungashintshwa ngomshini (kujikwe, kuhlelwe, kugaywe, njll.). Amandla aphezulu okucindezela. Ukumelana okuhle nokukhuhla okumaphakathi.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Electrode Yenduku Yokushisela EqinileURODO P

RODO PARA RECUBRIMIENTO UMVIKELI

Inombolo Yohlobo:B – 83

Ukuhlaziywa Kwensimbi Ediphozithiwe (Amanani ajwayelekile)

C

0.1%

Mn

0.9%

Si

0.8%

Cr

3.2%

 

Izici:

I-electrode ye-hydrogen ephansi yokushisela kabusha. Ukushisela kungashintshwa ngomshini (kujikwe, kuhlelwe, kugaywe, njll.). Amandla aphezulu okucindezela. Ukumelana okuhle nokukhuhla okumaphakathi.

 

Izakhiwo Zemishini:Ukuqina 27-31 HRc

 

Izikhundla Zokushisela:Isicaba, Esivundlile, Esiphezulu, Esiqonde Phezulu.

 

I-Current kanye ne-Polarity:

Kokushintshana noma okuqondile kwamanje

i-electrode kuya ensikeni enhle

ø mm

ø in

I-Amperage

3.20

1/8

110-130

4.00

5/32

140-180

5.00

2/16

190-240

 

Izicelo: Kuma-feed roller, ama-pulley, izicathulo zamabhuleki.

• Ukugcwalisa ama-sprockets ama-tractor

• Kuhle kakhulu njengesisekelo sezinto eziqinile ezimbozweni zensimbi yekhabhoni.

ikhabhoni

• Ama-trunnion, ama-axle kanye nama-caterpillar amafosholo omshini.

• Amasilinda okuchoboza

• Ama-Conveyor roller

 

 

UBUDE: 350mm.

ISINDI NGEBHOKISI: 20 kg/44 lbs.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besilokhu sihilelekile ekukhiqizenii-electrode yokushiselas, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 

 

 


  • Okwedlule:
  • Olandelayo: