I-Electrode Yokushisela Enezicabha Eziqinile DIN 8555 (E9-UM-250-KR) I-Electrode Yokushisela Enezicabha Ezinezinti, Izinduku Zokushisela Ezinamathelayo

Incazelo emfushane:

I-DIN 8555 (E9-UM-250-KR) iyi-electrode ekhethekile enezakhiwo zokushisela ezifanele kanye nezokukhanda. I-Austenite- Ferrites ishisela insimbi. Amanani aphezulu amandla kanye nokumelana okuphezulu kokuqhekeka.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Ukushisela OkuqinileI-electrode

Okujwayelekile: DIN 8555 (E9-UM-250-KR)

Inombolo Yohlobo: TY-C65

 

Ukucaciswa & Isicelo:   

· I-electrode ekhethekile enezakhiwo zokushisela ezifanele kanye nezakhiwo zemishini.

· I-Austenite- Ama-Ferrite ashisela insimbi. Amanani aphezulu okuqina kanye nokumelana okuphezulu kokuqhekeka.

· Ifaneleka kakhulu ukujoyina izinsimbi ezingashiseki kalula, lapho kudingeka kakhulu khona umthungo wokushisela.

· Ukumelana okukhulu kokuqhekeka lapho kuhlanganiswa izinsimbi zomzali ezilukhuni ukushibilika, njengezinsimbi ze-austenitic neze-ferritic, izinsimbi ze-manganese ezinezinsimbi ezixubile nezingaxubile, izinsimbi eziphathwa ngokushisa kanye nezamathuluzi. Izicelo ekulungisweni nasekugcinweni kwezingxenye zomshini kanye ne-drive kanye nasekulungisweni kwamathuluzi.

· Njengoba ungqimba lomcamelo kulezi zinto lufanelekile futhi.

 

 

Ukwakheka kwamakhemikhali kwensimbi egciniwe (%):

 

C

Si

Mn

P

S

Cr

Ni

Mo

N

Fe

I-DIN

-

0.15

-

0.90

0.50

2.50

-

0.04

-

0.03

28.0

32.0

8.0

10.0

-

-

Ibhalansi.

Okuvamile

0.1

1.0

1.0

≤0.035

≤0.025

29.0

9.0

≤0.75

0.10

Ibhalansi.

 

Ukuqina kwensimbi egciniwe:

Amandla okukhiqiza

I-Mpa

Amandla okudonsa

I-Mpa

Ukwelulwa

A(%)

Ubulukhuni Njengoba Buhlanganisiwe

(HB)

620

800

22

240

 

Izici Ezijwayelekile:

· Isakhiwo esincane i-Austenite + i-Ferrite

· Ukusebenza kahle kakhulu

· Ukufudumeza Ukufudumeza izingxenye ze-ferritic ezigobile ngodonga olujiyile ku-150-150℃