I-Electrode Yokushisela Eqinile Izinduku Zokushisela Ezingaphezulu DIN 8555 (E10-UM-60-GRZ) I-Electrode Yokushisela E-Arc

Incazelo emfushane:

I-DIN 8555 (E10-UM-60-GRZ) iyi-electrode ye-SMAW eyisisekelo embozwe nge-high recovery ephezulu yokufakelwa kwe-hardsurfacing.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Ukushisela OkuqinileI-electrode

 

Okujwayelekile: I-DIN 8555 (E10-UM-60-GRZ)

Inombolo Yohlobo: TY-C LEDURIT 61

 

Ukucaciswa & Isicelo:

· I-electrode ye-SMAW eyisisekelo ehlanganisiwe yokubuyisela i-hardsurfacing.

· Ubuso obuqinile kakhulu bezingxenye ezikhubeka kakhulu futhi zithinteka kancane.

· Kufanelekela izendlalelo zokugcina eziqinile ngemva kwesendlalelo se-buffer.

· Izingxenye zezitshalo ezisikiwe, imigoqo namapuleti agugile, imigoqo yokusikeka, i-blast furace, izinhlelo zokushaja, izitofu zesimende, amazinyo nezindebe zamabhakede, izikrini.

 

Ukwakheka kwamakhemikhali kwensimbi egciniwe (%):

 

C

Si

Mn

Cr

Mo

Nb

W

V

Ni

Fe

I-DIN

Okuqukethwe okuphezulu kwe-C kanye nokuqukethwe kwe-Cr

Ibhalansi.

EN

1.5

4.5

-

0.5

3.0

25

40

-

4.0

-

-

-

-

4.0

Ibhalansi.

Okuvamile

3.2

1.0

1.8

29

-

-

-

-

-

Ibhalansi.

 

 

Ukuqina kwensimbi egciniwe:

Njengoba Kushiselwe

(HRC)

Isendlalelo esi-1 ensimbini eno-C=0.15%

(HRC)

Isendlalelo esingu-1 ensimbini ephezulu ye-Mn

(HRC)

60

55

52

 

Izici Ezijwayelekile:

· Isakhiwo esincane se-Martensitic+Austenite+Carbides

· Ukugaya Okusebenziseka Kalula kuphela

· Uku-Retry i-Redry amahora ama-2 ku-300℃ ngaphambi kokusebenzisa.

 