Induku Yokushisela Yensimbi Ene-Alloy Ephansi AWS E8018-G (J556Fe) Manual Metal Arc Electrodes

Incazelo emfushane:

I-J556Fe (AWS E8018-G) iyi-electrode yensimbi e-alloy ephansi enempuphu yensimbi kanye ne-hydrogen ephansi. Kokubili i-AC ne-DC kungasetshenziswa, futhi kungashiselwa kuzo zonke izikhundla.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Electrode Yokushisela Yensimbi Ephansi Ye-Alloy

J556Fe                                              

I-GB/T E5518-G

I-AWS E8018-G 

Incazelo: I-J556fe iyi-electrode yensimbi e-alloy ephansi enempuphu yensimbi kanye ne-hydrogen ephansi. Kokubili i-AC ne-DC kungasetshenziswa, futhi kungashiselwa kuzo zonke izikhundla.

Isicelo: Isetshenziselwa ukushisela insimbi ye-carbon ephakathi nendawo kanye nezakhiwo zensimbi ezi-alloy eziphansi njenge-Q390.

 

Ukwakheka kwamakhemikhali kwensimbi eshidiwe (%):

C

Mn

Si

S

P

≤0.12

≥1.00

≤0.80

≤0.035

≤0.035

 

Izakhiwo zemishini zensimbi yokushisela:

Into yokuhlola

Amandla okudonsa

I-Mpa

Amandla okukhiqiza

I-Mpa

Ukwelulwa

%

Inani lomthelela (J)

-40℃

Kuqinisekisiwe

≥540

≥440

≥17

≥27

 

Okuqukethwe kwe-hydrogen okusabalala kwensimbi egciniwe: ≤10.0mL/100g (indlela ye-mercury noma i-gas chromatography)

Ukuhlolwa kwe-X-ray: Ibanga lokuqala

 

I-current enconyiwe:

(mm)

Ububanzi benduku

2.5

3.2

4.0

5.0

(A)

Ukushisela Kwamanje

70 ~ 110

100 ~ 140

140 ~ 170

190 ~ 240

 

Isaziso:

1. I-electrode kumele ibhakwe ihora eli-1 ku-350℃ ngaphambi kokusebenza kokushisela;

2. Kubalulekile ukuhlanza izikali zikawoyela, amanzi kanye nokungcola okugqwalile ezingxenyeni zokushisela ngaphambi kokushisela;

3. Sebenzisa umsebenzi omfushane we-arc lapho ushisela. Indlela encane yokushisela ifanelekile.

 