I-Electrode Yokushisela Yensimbi Ephansi Ye-Alloy
J506NiMA、J507NiMA
I-GB/T E5016-G E5015-G
I-AWS E7018-G E7015-G
Incazelo: I-J506NiMA kanye ne-J507NiMA ziyi-electrode zensimbi ezithambile ezimunca umswakama ezimbozwe nge-hydrogen ephansi kakhulu. Insimbi efakiwe inobucwebe obuhle kakhulu, ukuqina kwezinga lokushisa eliphansi kanye nokumelana nokuqhekeka, futhi ingashiselwa kuzo zonke izikhundla. Ingubo imelana nokumuncwa komswakama. Ngemva kokuba i-electrode ibhakiwe ku-400°C x ihora eli-1 futhi ipakwe endaweni enomswakama olinganiselwe ≥ 80% amahora ama-4, okuqukethwe komswakama kwengubo kusahlangabezana nezidingo zokusetshenziswa.
Isicelo: Isetshenziselwa ukushisela amapulatifomu kawoyela, imikhumbi, imikhumbi yokucindezela, nezinye izakhiwo ezenziweinsimbi yekhabhoni kanye nensimbi ephansi ye-alloy.
Ukwakheka kwamakhemikhali kwensimbi eshidiwe (%):
| C | Mn | Si | Ni | S | P | |
| Kuqinisekisiwe | ≤0. 12 | ≥1.00 | ≤0.50 | ≤0.60 | ≤0.035 | ≤0.040 |
Izakhiwo zemishini zensimbi yokushisela:
| Into yokuhlola | Amandla okudonsa I-Mpa | Amandla okukhiqiza I-Mpa | Ukwelulwa % | Inani lomthelela (J) -46℃ |
| Kuqinisekisiwe | ≥490 | ≥390 | ≥22 | ≥27 |
Okuqukethwe kwe-hydrogen okusabalala kwensimbi egciniwe: ≤5.0mL/100g (i-gas chromatography noma indlela ye-mercury)
Okuqukethwe komswakama kwezembozo ze-electrode: ≤0.30%
Ukuhlolwa kwe-X-ray: Ibanga lokuqala
I-current enconyiwe:
| Ububanzi benduku | 2.5 | 3.2 | 4.0 | 5.0 |
| Ukushisela Kwamanje | 60 ~ 90 | 90 ~ 120 | 140 ~ 180 | 170 ~ 210 |
Isaziso:
1. I-electrode kumele ibhakwe ihora eli-1 ku-350 ~ 400℃ ngaphambi kokusebenza kokushisela;
2. Kubalulekile ukuhlanza izikali zikawoyela, amanzi kanye nokungcola okugqwalile ezingxenyeni zokushisela ngaphambi kokushisela;
3. Sebenzisa umsebenzi omfushane we-arc lapho ushisela. Indlela encane yokushisela ifanelekile.