Intambo Yokushisela ye-Nickel Alloy Intambo ye-ERNiCrMo-4 Tig

Incazelo emfushane:

I-ER-NiCrMo-4 isetshenziselwa ukushisela ama-alloy anezakhi zamakhemikhali ezifanayo, lokhu kufaka phakathi izinto ezingafani zama-alloy e-nickel-base, izinsimbi kanye nezinsimbi ezingagqwali.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Nickel AlloyUcingo LokushiselaIntambo yeTigI-ERNiCrMo-4

 

Amazinga
I-EN ISO 18274 – Ni 6276 – NiCr15Mo16Fe6W4
I-AWS A5.14 – ER NiCrMo-4

 

Izici kanye nezinhlelo zokusebenza

I-ER-NiCrMo-4 isetshenziselwa ukushisela ama-alloy anezakhi zamakhemikhali ezifanayo, lokhu kufaka phakathi izinto ezingafani ze-i-nickel-izinsimbi eziyisisekelo, izinsimbi kanye nezinsimbi ezingagqwali.

Ngenxa yokuqukethwe okuphezulu kwe-molybdenum, le ngxubevange inikeza ukumelana okuhle kakhulu nokucindezeleka kanye nokuqhekeka kokugqwala, ukugqwala kwemigodi kanye nokugqwala kwemifantu.

Ngokuvamile isetshenziswa kumapayipi, imikhumbi yokucindezela, izikhungo zokucubungula amakhemikhali, amapulatifomu kawoyela asogwini, izikhungo zegesi, ukukhiqizwa kukagesi kanye nezindawo zasolwandle njll.

Izinto Eziyisisekelo Ezijwayelekile

N10276, W.Nr: 2.4819, NiMo16Cr15W, Ingxubevange C4, Ingxubevange C276*
* Uhlu olubonisayo, hhayi oluphelele

 

 

Ukwakheka Kwamakhemikhali %
C% Mn% I-Fe% P% S% I-Si%  
ubuningi ubuningi ubuningi ubuningi ubuningi ubuningi  
0.05 0.80 0.70 0.030 0.010 0.75  
             
I-Cu% I-Ni% I-Co% I-Ti% I-Al%    
ubuningi 93.00 ubuningi 2.00 ubuningi    
0.20 umzuzu 1.00 3.50 1.00    

 

Izakhiwo Zemishini
Amandla Okudonsa ≥690 MPa  
Amandla Okukhiqiza -  
Ukwelulwa -  
Amandla Omthelela -  

Izakhiwo zemishini ziyalinganiselwa futhi zingahluka ngokuya ngokushisa, igesi yokuvikela, amapharamitha okushisela kanye nezinye izici.

 

Amagesi Okuvikela

I-TS EN ISO 14175 TIG: I1 (Argon)

 

Izikhundla Zokushisela

I-TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Idatha Yokupakisha
Ububanzi Ubude Isisindo  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

Isibopho: Nakuba kwenziwe yonke imizamo efanelekile ukuqinisekisa ukunemba kolwazi oluqukethwe, lolu lwazi lungashintsha ngaphandle kwesaziso futhi lungabhekwa njengolufanelekela isiqondiso esijwayelekile.