I-AWS A5.23: Umhlinzeki Wezinto Ezisetshenziswayo Zokushisela I-Arc Ecmerged ECM4

Incazelo emfushane:

I-AWS A5.23: I-ECM4 Submerged Arc Solid Wire iyi-electrode yensimbi ehlanganisiwe ene-alloy ephansi yokushisela i-arc engaphansi kwe-submerged ezisetshenziswayo zamandla aphezulu. I-AWS A5.23: I-ECM4 ihlangabezana ne-AWS A5.23 chemistry M4, futhi yenzelwe amazinga amandla okudonswa angaphezu kuka-110 ksi.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

INCAZELO:

Izintambo Ezine-Arc Cored Ezicwiliswe Emanzini Insimbi Ephansi Ye-Alloy

ISIGABA:

I-AWS A5.23: I-ECM4 Submerged Arc Solid Wire iyi-electrode yensimbi ehlanganisiwe ene-alloy ephansi yokushisela i-arc engaphansi kwe-submerged ezisetshenziswayo zamandla aphezulu. I-AWS A5.23: I-ECM4 ihlangabezana ne-AWS A5.23 chemistry M4, futhi yenzelwe amazinga amandla okudonswa angaphezu kuka-110 ksi.

ISICELO ESIYINHLOKO:

Izicelo zokudlula okukodwa noma okuningi nge-arc flux engaphansi kwamanzi enconyiwe, izinsimbi ze-High-Strength Low-Alloy, izinsimbi ze-Quinch & Tempered, Izingxenye zemishini esindayo, izingxenye zesakhiwo, ama-ship hulls, izinsimbi ze-cast, imikhumbi ye-boiler kanye ne-pressure

Izinsimbi ze-HSLA kanye ne-Q&T

Ukwakhiwa kwesakhiwo

Ukwenziwa kwemishini ye-Jack-up

Ozimele bemishini esindayo

Imisebe ye-crane

EZIPHUMA:

Intambo ene-metal-core inganikeza amazinga okubekwa athuthukisiwe uma kuqhathaniswa nezintambo eziqinile kuma-amperage afanayo

Izintambo ezine-core yensimbi zinikeza amaphrofayili amaningi okungena uma kuqhathaniswa nezintambo eziqinile kumapharamitha okushisela afanayo

Idiphozithi enamandla aphezulu kakhulu enokuqina okuhle kakhulu kwezinga lokushisa eliphansi esimweni esishisiwe

Izidingo ze-weld deposit chemistry ziyafana nezezintambo eziqinile ze-EM4

UKUHLELA KWE-AWS:

Nge-Flux Isimo Imininingwane Ukuhlukaniswa (Amayunithi Angokwesiko ase-US) Ukuhlukaniswa (Amayunithi e-SI)
I-SWX 150 Njengoba Kushiselwe A5. 23/A5 23M F11A10-ECM4-M4 F76A7-ECM4-M4
Nge-Flux %C % Mn %Si %P %S % Cu % Cr % Ni % Mo %TI+V+Zr
I-SWX 150 0.06 1.45 0.27 0.012 0.010 0.06 0.31 2.25 0.47 0.02

UKWAKHIWA KWAMAKHEMIKHALI OKUJWAYELEKILE OKUNGENA:

Nge-Flux I-Hydrogen Esakazekayo
I-SWX 150 7.5 ml/100g

IZINDAWO EZIJWAYELEKILE ZOMKHIQIZO:

Nge-Flux Isimo Amandla Okudonsa Amandla Okukhiqiza Ukuphakama okungu-% ku-2" (50 mm)
I-SWX 150 Njengoba Kushiselwe 113 ksi (779 MPa) 106 ksi (731 MPa) 20%
I-PWHT* 104 ksi (717 MPa) 97 ksi (669 MPa) 8%

AMANINGI OMTHELELA OKUJWAYELEKILE E-CHARPY V-NOTCH:

Nge-Flux Isimo Isilinganiso ku--60°F (-50°C) Isilinganiso ku--80°F (-60°C) Isilinganiso ku--100°F (-70°C)
I-SWX 150 Njengoba Kushiselwe 55 ft-lbs (75 J) Ama-f-bs angu-60 (81 J) 45 f-Ibs (61 J)
I-PWHT* 57 f-lbs (77 J) 45 ft-lbs (61 J) —

AMAPHARAMETHI OKUSEBENZA AJWAYELEKILE: