Incazelo emfushane:

I-A022 (AWS A5.4 E316L-16) i-ultra-low carbon Cr18Ni12Mo2 electrode yensimbi engagqwali ene-titanium calcium coating.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

Stainless Steel Welding Electrode

A022                                                 

I-GB/T E316L-16

I-AWS E316L-16

Incazelo: I-A022 iyi-electrode yensimbi engenasici ene-ultra-low carbon Cr18Ni12Mo2 ene-titanium calcium coating.Ingasetshenziselwa kokubili i-AC ne-DC ngokusebenza kahle kwenqubo.Okuqukethwe kwekhabhoni yensimbi efakiwe ngu-≤0.04%, okuyihlinzeka ngokumelana nokushisa okuhle, ukumelana nokugqwala kanye nokumelana nokuqhekeka.

 Isicelo: Isetshenziselwa ukushisela i-urea, i-synthetic fiber nezinye izinto zokusebenza kanye nohlobo olufanayo lwesakhiwo sensimbi engagqwali.Ingase futhi isetshenziselwe i-chromium insimbi engagqwali, insimbi eyinhlanganisela kanye nensimbi ehlukile engakwazi ukuphathwa ngokushisa ngemva kokushisela.

 

Ukwakheka kwamakhemikhali ensimbi ye-weld(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Izici zemishini ye-weld metal:

Into yokuhlola

Amandla aqinile

Mpa

Ukwelula

%

Kuqinisekisiwe

≥490

≥30

 

Okwamanje okunconyiwe:

Ububanzi benduku

(mm)

2.0

2.5

3.2

4.0

5.0

I-Welding Yamanje

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode kufanele ibhakwe ihora elingu-1 endaweni engaba ngu-150 ℃ ngaphambi kokusebenza kokushisela;

2. Ngenxa yokuthi ukujula kokungena akujulile ngesikhathi sokushisela i-AC, amandla kagesi e-DC kufanele asetshenziswe ngangokunokwenzeka ukuze uthole ukungena okujulile.futhi umsinga akufanele ube mkhulu kakhulu ukugwema ukubomvu kwenduku yokushisela;

3.Ukumelana nokugqwala kwensimbi efakwe kunqunywa isivumelwano esiphindwe kabili sokuhlinzeka nokufunwa.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesineminyaka engaphezu kwengu-20 sisebenza ekwenzeni ama-welding electrode, izinduku zokushisela, nezinto ezisetshenziswayo zokushisela.

Imikhiqizo yethu eyinhloko ihlanganisa ama-electrode ensimbi engagqwali, ama-electrode welding steel, i-low alloy welding electrode, ama-electrode welding angaphezulu, ama-electrode welding we-nickel & cobalt alloy, izintambo zokushisela zensimbi emnene & ne-alloy ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe igesi eziguquguqukayo, izintambo zokushisela i-aluminium, i-arc welding engaphansi kwamanzi.izintambo, izintambo zokushisela i-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode ama-tungsten, ama-electrode okugobhoza ikhabhoni, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 


  • Okwedlule:
  • Olandelayo: