I-AWS E7014 I-Carbon Steel Welding Electrodes J501Fe Mild Steel Welding Rods

Incazelo emfushane:

I-J501Fe (AWS E7014) iyimpushana yensimbi kanye nohlobo lwe-titanium oxide embozwe i-electrode.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Carbon Steel Welding Electrode

J501Fe

I-GB/T E5014

I-AWS A5.1 E7014

Incazelo: I-J501Fe iyimpushana yensimbi kanye nohlobo lwe-titanium oxide embozwe i-electrode.Ingasetshenziselwa ukushisela yonke indawo nge-AC ne-DC, ukusebenza kahle kwe-deposition cishe ku-110%.

Isicelo: Ukuze carbon steel kanye low ingxubevange steel izakhiwo, ezifana Q345 kanye neminye imikhumbi, izimoto kanye mechanical izakhiwo Welding.

Ukwakheka kwamakhemikhali ensimbi ye-weld(%):

C

Mn

Si

S

P

≤0.12

≤1.25

≤0.60

≤0.035

≤0.035

 

Izici zemishini ye-weld metal:

Into yokuhlola

Amandla aqinile

Mpa

Amandla esivuno

Mpa

Ukwelula

%

Inani lomthelela (J)

0℃

Kuqinisekisiwe

≥490

≥400

≥17

≥27

Ihloliwe

520 ~ 580

≥410

17-26

50 ~ 100

 

Ukuhlolwa kwe-X-ray: II grade

Okwamanje okunconyiwe:

Ububanzi benduku

(mm)

2.0

2.5

3.2

4.0

5.0

5.8

Welding current

(A)

40 ~ 70

70 ~ 90

90 ~ 130

160 ~ 210

210 ~ 250

260 ~ 310

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesineminyaka engaphezu kwengu-20 sisebenza ekwenzeni ama-welding electrode, izinduku zokushisela, nezinto ezisetshenziswayo zokushisela.

Imikhiqizo yethu eyinhloko ihlanganisa ama-electrode ensimbi engagqwali, ama-electrode welding steel, i-low alloy welding electrode, ama-electrode welding angaphezulu, ama-electrode welding we-nickel & cobalt alloy, izintambo zokushisela zensimbi emnene & ne-alloy ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe igesi eziguquguqukayo, izintambo zokushisela i-aluminium, i-arc welding engaphansi kwamanzi.izintambo, izintambo zokushisela i-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode ama-tungsten, ama-electrode okugobhoza ikhabhoni, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 


  • Okwedlule:
  • Olandelayo: