I-AWS E7015-G I-Low Temperature Welding Electrode W607 Low-Hydrogen Welding Rod

Incazelo emfushane:

I-W607 (AWS E7015-G) iyi-electrode yensimbi enezinga lokushisa eliphansi ene-low-hydrogen sodium coating.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Low Temperature Steel Welding Electrode

W607                                                     

I-GB/T E5015-G

I-AWS A5.5 E7015-G

 

Incazelo: I-W607 iyi-electrode yensimbi enezinga lokushisa eliphansi ene-low-hydrogen sodium coating.Sebenzisa i-DCEP (i-electrode yamanje eqondile) futhi ingashiselelwa kuzo zonke izikhundla.Insimbi efakiwe inokuqina okuhle komthelela ku -60°C.

Isicelo: Isetshenziselwa ukushisela insimbi yokushisa ephansi efana ne-09MnD.

 

Ukwakheka kwamakhemikhali ensimbi ye-weld(%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.65

≤0.60

0.50 ~ 2.50

≤0.020

≤0.025

 

Izici zemishini ye-weld metal:

Into yokuhlola

Amandla aqinile

Mpa

Amandla esivuno

Mpa

Ukwelula

%

Inani lomthelela (J)

-60 ℃

Kuqinisekisiwe

≥490

≥390

≥22

≥27

 

Okuqukethwe kwe-hydrogen yokusabalalisa kwensimbi efakiwe: ≤6.0mL/100g (indlela ye-glycerin) noma ≤10mL/100g (i-mercury noma indlela ye-gas chromatography)

Ukuhlolwa kwe-X-ray: I grade

 

Okwamanje okunconyiwe:

(mm)

Ububanzi benduku

2.0

2.5

3.2

4.0

5.0

(A)

I-Welding Yamanje

40 ~ 70

60 ~ 90

100 ~ 120

140 ~ 170

170 ~ 200

 

Isaziso:

1. I-electrode kufanele ibhakwe ihora elingu-1 ku-350 ℃ ngaphambi kokusebenza kokushisela;

2. Kubalulekile ukuhlanza okugqwalile, isikali sikawoyela, amanzi, nokungcola ezingxenyeni zokushisela ngaphambi kokushisela;

3. Ingxenye eshiselwe ingashiswa ngaphambi kuka-150 ° C ngaphambi kokushisela ukuvimbela ukuqhekeka.

 