I-AWS E9015-G I-Low Alloy Steel Welding Rod Okuphansi kwe-hydrogen Welding Electrodes J607CrNiMo

Incazelo emfushane:

I-J607CrNiMo (AWS E9015-G) i-electrode yensimbi ephansi ye-alloy ene-sodium ephansi ye-hydrogen coating.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Electrode ephansi ye-Alloy Steel Welding

I-J607CrNiMo                                       

I-GB/T E6015-G

I-AWS E9015-G

 

Incazelo: I-J607CrNiMo i-electrode yensimbi ephansi ene-hydrogen ephansi ene-sodium coating.Sebenzisa i-DCEP (i-electrode yamanje eqondile eqondile), futhi ingashiselwa kuzo zonke izikhundla ngokusebenza kwe-arc emfushane.Induku yokushisela inokujula okukhulu kokungena, i-spatter encane nokusebenza okuhle kokusebenza.Insimbi ediphozithi ine-plasticity enhle, izinga lokushisa eliphansi eliqinile kanye nokumelana nokuqhekeka.

Isicelo: Isetshenziselwa ukushisela amapayipi okuhambisa amanzi angaphansi kuka-350 °C eziteshini zikagesi nezinsimbi zemikhumbi yokucindezela ezinamabanga ahambisanayo amandla.Inofanelana kahle nensimbi yasekhaya ye-WB36CN1 (HD15Ni1MnMoNbCu), futhi ifanele ukushisela insimbi ye-WB3 (15NiCuMoNb5).

 

Ukwakheka kwamakhemikhali ensimbi ye-weld(%):

C

Mn

Si

Cr

Ni

Mo

S

P

≤0.10

1.00 ~ 1.60

≤0.50

0.14 ~ 0.35

0.60 ~ 1.20

0.15 ~ 0.50

≤0.015

≤0.015

 

Izici zemishini ye-weld metal:

Into yokuhlola

Amandla aqinile

Mpa

Amandla esivuno

Mpa

Ukwelula

%

Inani lomthelela (J)

-30 ℃

Kuqinisekisiwe

620 ~ 720

≥500

≥20

≥47

 

Okuqukethwe kwe-hydrogen yokusabalalisa kwensimbi efakiwe: ≤5.0mL/100g (i-mercury noma indlela ye-gas chromatography)

Ukuhlolwa kwe-X-ray: I grade

 

Okwamanje okunconyiwe:

(mm)

Ububanzi benduku

3.2

4.0

5.0

(A)

I-Welding Yamanje

100 ~ 140

140 ~ 18

190 ~ 230

 

Isaziso:

1. I-electrode kufanele ibhakwe ihora elingu-1 endaweni engaba ngu-350 ℃ ngaphambi kokusebenza kokushisela;

2. Kubalulekile ukuhlanza okugqwalile, isikali sikawoyela, amanzi, nokungcola ezingxenyeni zokushisela ngaphambi kokushisela.