I-AWS ENi-C1 (Z308) I-Pure Nickel Cast Iron Welding Electrode I-Nickel 99 Welding Rods I-Arc Stick Electrodes Ni99

Incazelo emfushane:

I-AWS ENi-C1 (Z308) iyi-electrode yensimbi ephonswe ngensimbi enomongo wensimbi enekhabhoni ephansi kanye noqweqwe oluqinile olune-graphitized.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Electrode Yokushisela Insimbi Ephonswe Ngensimbi

I-Z308                                                     

I-GB/T EZNi-1

I-AWS A5.15 ENi-C1

Incazelo: I-Z208 iyi-electrode yensimbi ephothiwe ene-core yensimbi ephansi yekhabhoni kanye ne-graphitized coating eqinile. Ingasetshenziswa kokubili i-AC kanye ne-DC. I-weld ingaba yi-cast iron empunga uma ipholiswa kancane, kodwa ukumelana kwayo nokuqhekeka akubi.

Ukusetshenziswa: Kusetshenziselwa ukulungisa amaphutha kuma-grey iron castings.

 

Ukwakheka kwamakhemikhali kwensimbi eshidiwe (%):

C

Si

Mn

S

Ni

Fe

Abanye

≤2.0

≤2.5

≤1.0

≤0.03

≥90

≤8.0

≤1.0

 

I-current enconyiwe:

Ububanzi benduku

(mm)

2.5

3.2

4.0

Ukushisela okwamanje

(A)

65 ~ 90

90 ~ 110

120 ~ 150

 

Isaziso:

1. I-electrode kumele ibhakwe ihora eli-1 cishe ngo-150℃ ngaphambi kokusebenza kokushisela;

2. Ukucindezeleka endaweni yokulungisa ukushisela kungaqedwa ngokushaya i-weld ukuze kugwenywe imifantu.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 


  • Okwedlule:
  • Olandelayo: