I-AWS ENiFe-C1 (Z408) I-Pure Nickel Cast Iron Welding Electrodes I-Nikel 55 Welding Rods

Incazelo emfushane:

I-AWS ENiFe-C1 (Z408) iyi-electrode yensimbi ephonswe ngensimbi enomongo we-nickel alloy kanye ne-graphitized coating. I-AC ne-DC enezinjongo ezimbili, i-arc ezinzile, kulula ukuyisebenzisa.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

IZICELO:

Ifanele ukushisela insimbi empunga enamandla aphezulu kanye nensimbi ehlanganisiwe enezimbotshana, njengesilinda, ibhulokhi yenjini, ibhokisi legiya, njll.

UKUHLELA:

I-AWS A5.15 / ASME SFA5.15 ENiFe-CI

I-JIS Z3252 DFCNiFe

IZIMALI:

I-AWS ENiFe-CI (Z408) iyi-electrode yensimbi ehlanganisiwe ene-nickel iron alloy core kanye nokunciphisa okukhulu kwe-graphite coating. Ingasetshenziswa ku-AC kanye ne-DC dual purpose, ine-arc ezinzile, futhi kulula ukuyisebenzisa. I-electrode inezici zamandla aphezulu, i-plasticity enhle, i-low linear expansion coefficient njalo njalo. Ukumelana nokuqhekeka kwensimbi ehlanganisiwe empunga kufana nalokho kwe-Z308, kanti ukumelana nokuqhekeka kwensimbi ehlanganisiwe empunga kungaphezu kwe-ENi-CI (Z308). Ngensimbi ehlanganisiwe ene-phosphorus ephezulu (0.2%P), nayo inemiphumela emihle futhi ukusebenza kwayo kokusika kuphansi kune-Z308 kanye ne-Z508 kancane. I-Z408 isetshenziswa ekuhlanganiseni insimbi ehlanganisiwe empunga kanye nensimbi ehlanganisiwe empunga endaweni.

QAPHELA:

Ngaphambi kokushisela, ama-electrode kudingeka abhakwe ihora eli-1 ngokushisa okungu-150±10℃ ngaphambi kokusebenzisa.

Uma ushisela, kufanelekile ukuthatha i-weld encane futhi ubude be-weld ngayinye akufanele budlule u-50mm. Shaya indawo yokushisela kancane ngesando ngokushesha ngemva kokushisela ukuze ususe ukucindezeleka futhi uvimbele imifantu.

Kunconywa ukufaka ukushisa okuphansi.

UKUBUMBEKA KWAMAKHEMIKI YENSIMBI EDIPHIWE (INGXENYE ENKULU): %

Izinto

C

Si

Mn

S

Fe

Ni

Cu

Ubuningi bezinye izakhi

Inani elijwayelekile

0.35-0.55

≤0.75

≤

2.3

≤0.025

3.0-

6.0

60-

70

25-

35

≤

1.0

ISITHEMBISO SOKUSHINTSHA NGOKUSHINTSHA:(AC,DC+)

Ububanzi be-electrode (mm)

3.2

4.0

5.0

Ubude (mm)

350

350

350

Ukushisela kwamanje (A)

90-110

120-150

160-190

Izici Zokusetshenziswa:

I-arc eqinile kakhulu.

Ukususwa okuhle kakhulu kwe-slag.

Ukungena akujulile.

Ukumelana okuhle nokushisa nokugqwala.

Ukumelana okuhle kakhulu nokuqhekeka.


  • Okwedlule:
  • Olandelayo: