Izintambo Zokushisela Zensimbi Engagqwali ze-AWS ER347 MIG kanye Nezintambo Zokushisela ze-TIG

Incazelo emfushane:

Intambo yokushisela yensimbi engagqwali isebenza kahle kakhulu ekushiseleni, ukusebenza kahle kobuchwepheshe bokushisela ezindaweni zonke. Zisetshenziswa kabanzi embonini: izakhiwo zokwakha, izimoto, ubunjiniyela bamabhuloho, imishini yezimayini, izitimela, amapayipi kawoyela, imishini ephethe umfutho wegesi, imishini kagesi, njll.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Ukuhlukaniswa kwe-AWS: AWS 5.9

INCAZELO:

Intambo yokushisela yensimbi engagqwali inokusebenza kahle kakhulu kokumboza, ukusebenza kahle kobuchwepheshe bokushisela ekushiseleni okunezindawo zonke. Zisetshenziswa kabanzi embonini: isakhiwo sesakhiwo, izimoto, ubunjiniyela bebhuloho, imishini yezimayini, izitimela, ipayipi likawoyela, imishini ephethe umfutho wegesi, imishini kagesi, njll.

INOMBOLO YEMODELO NOSAYIZI:

1. Insizakalo ye-OEM yokunikezwa kwefektri.

2. Imodeli: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi njll.

3. Usayizi wentambo ye-MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4. Usayizi wentambo ye-TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm .

ISINGENISO:

Sihlinzeka ngezinhlobo ezahlukene zocingo lokushisela lwensimbi engagqwali, okuhlanganisa ucingo lokushisela lwe-Mig solid, ucingo lokushisela lwe-Tig rod kanye nocingo lokushisela olungaphansi kwe-arc, zonke zisezingeni eliphezulu futhi zithengiswa emhlabeni jikelele.

Ngaphandle kwe-308 ne-309, siphinde sinikeze i-304, 321, 347, 316L, 310, 2209, kanye ne-201. Kanye nemininingwane ekhethekile efana ne-318L, 904L, 2594, NiCrMo-3, Ni1.

UKUPHAKISHA:

Ukupakisha ucingo lokushisela i-Mig (iphakethe le-spool kanye ne-drum)

Ububanzi: 0.8 - 2.0mm

Iphakheji: 1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/drum, 200 kg/drum

Ukupakisha ucingo lokushisela induku ye-tig (ipayipi lepulasitiki)

Ububanzi: 1.0 - 5.0mm

Iphakheji: 5 kg/iphakethe

Ucingo lokushisela lwe-arc olucwiliswe emanzini

Ububanzi: 2.5 - 5.0mm

Iphakheji: 20kg/iphakethe, 25 kg/iphakethe

Ukupakisha okungathathi hlangothi kanye ne-OEM kwamukelekile!

IZINHLANGANO ZAMAKHEMIKI EZINTAMBO ZOKUSHINTSHA EZINGAKAGQI:

Inombolo Yemodeli

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

I-ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

I-ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

I-ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

I-ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

I-ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

I-ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

I-ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

I-ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

I-ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

I-ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

I-ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

I-ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

I-ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

I-ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

IZIMPAHLA ZOKUSHINTSHA NGOCINGO LOKUSHINTSHA:

Inombolo Yemodeli

Amandla okudonsa i-Rm(Mpa)

Amandla okukhiqiza i-Rel noma i-Rp0.2(Mpa)

Ukwelulwa

(%)

Inombolo Yemodeli

Amandla okudonsa i-Rm(Mpa)

Amandla okukhiqiza i-Rel noma i-Rp0.2(Mpa)

Ukwelulwa

(%)

304

550

--

25

I-ER309LSi

510

320

25

304L

510

--

25

I-ER316

510

320

25

I-ER307

590

350

25

I-ER316L

510

320

25

I-ER308

550

350

25

I-ER316LSi

510

320

20

I-ER308L

510

320

25

I-ER310

550

350

25

I-ER308LSi

510

320

25

I-ER347

550

350

25

I-ER309

550

350

25

I-ER317

550

350

25

I-ER309L

510

320

25

I-ER321

550

350

25

Ukwakheka kwentambo yokushisela yensimbi engagqwali ye-TIG ne-MIG

YB5092-2005

I-AWS

Ukwakheka Kwamakhemikhali %

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

I-ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

I-ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

I-ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

I-ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

I-ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

I-ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

I-ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

I-ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

I-ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

I-ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

I-ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

I-ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

I-ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

I-ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

I-ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Inombolo 0.7

H02Cr20Ni34Mo2Cu3Nb

I-ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Inombolo 0.35

H08Cr20Ni10Ti

I-ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

I-Ti9xC-1.0

H08Cr21 Ni10Nb

I-ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

I-Nb1xC-1.0

H12Cr26Ni21

I-ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

I-ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

I-Cu 1.80

H03Cr22Ni9Mo3N

I-ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

I-ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

I-ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

H03Cr24Ni13MoL

I-ER309L Mo

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

I-ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

I-Cu;3 Nb;0.28

H08Cr26Ni5Mo2

Ama-ER453

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

I-ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N;0.20 V;0.18

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.


  • Okwedlule:
  • Olandelayo: