Intambo Yokushisela Yensimbi Engagqwali Ye-Flux Cored ye-E2209T1-1/T1-4

Incazelo emfushane:

Yenzelwe ukushisela endaweni ethile, kokubili phezulu phezulu kanye nomsebenzi wamapayipi ozinzile ofanelekela izikhundla zokushisela ze-ASME 5G noma ze-6G (ipayipi ngokuvamile liyi-> ububanzi obuyi-150mm,> udonga oluyi-15mm).
Bushelela ukushibilika kwesikhundla sonke


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Ikilasi le-AWS E2209T1-1/T1-4Intambo Eyinhloko Ye-Flux

IZICI
Ilungiselelwe ukushisela endaweni, kokubili phezulu phezulu kanye nomsebenzi wamapayipi ozinzile ofanelekela izikhundla zokushisela ze-ASME 5G noma ze-6G (ipayipi ngokuvamile liyi-> ububanzi obuyi-150mm,> udonga oluyi-15mm).
Bushelela ukushibilika kwesikhundla sonke
Ukususwa kwe-slag okuhle kakhulu

Igesi Yokuvikela
80% Argon / 20% CO2
I-CO2 engu-100%

Izici Eziyinhloko
• Hlehlisa ukushibilika kwesikhundla sonke
• Iphakethe elivaliwe nge-vacuum
• Ukususwa kwe-slag okuhle kakhulu
• Isitifiketi esibonisa ukwakheka kwediphozithi, inombolo ye-ferrite, kanye nezakhiwo ze-charpy impact ezihlolwe ku--196°C (-320°F)

Ikilasi le-AWS E2209T1-1/T1-4Intambo Eyinhloko Ye-FluxUkwakheka Kwamakhemikhali

C Cr Ni Mo Mn Si P S N Cu
.03 22.5 9.7 3.25 0.95 .60 0.03 .015 0.14 0.20
Izakhiwo Zomshini Wezintambo Ze-AWS Class E2209T1-1/T1-4 Flux Core
Amandla Okudonsa 120,000 psi
Amandla Okukhiqiza 95,000 psi
Ukwelulwa (%) 26%
Amapharamitha e-AWS Class E2209T1-1/T1-4 Flux Core Wire
Ububanzi I-WFS (ipm) I-Amperage Ama-volts I-ESO (ngaphakathi) Izinga Lokufaka Imali
(amakhilogremu/ihora)
.045” 250 130 22 5/8-3/4” 5.4
300 160 24 5/8-3/4” 6.3
425 200 26 5/8-3/4” 9.2
780 270 32 5/8-3/4” 16.2
1/16” 150 170 23 3/4-1” 5.4
195 215 25 3/4-1” 7.0
240 250 26 3/4-1” 8.6
320 305 27 3/4-1” 11.5

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besilokhu sihilelekile ekukhiqizeni ama-electrode okushisela,izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.


  • Okwedlule:
  • Olandelayo: