E2553T1-1/4 AP Stainless Steel Flux Cored Welding Wire

Incazelo emfushane:

I-E2553T1-4 AP intambo ene-flux-cored isetshenziselwa ukuhlanganisa ama-alloys ensimbi engagqwali e-duplex cishe cishe no-25% we-Chromium.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

E2553T1-1/4 AP FLUX-CORED WIRE

UKUHLUKANA
AWS 5.22 Ikilasi E2553T1-1 kanye E2553T1-4 / ASME SFA 5.22 Ikilasi E2553T1-1 kanye E2553T1-4
UNS# W39533 A#8 F#6

DESCRIPTION
I-E2553T1-4 intambo enezimbobo zonke eklanyelwe ukusebenza ku-75% Ar / 25% CO2.
Le ntambo yakhelwe ukuthi ibe nokususwa kwe-slag okuhle kakhulu futhi isebenza ngokudluliswa kwe-globular kwamahhala.

IZICELO
I-E2553T1-4 AP intambo ene-flux-cored isetshenziselwa ukuhlanganisa ama-alloys ensimbi engagqwali e-duplex cishe cishe no-25% we-Chromium.
Lawa ma-alloys ensimbi engagqwali ayi-duplex ahlanganisa ukushuba okuphezulu namandla akhiqizayo nokumelana okuthuthukisiwe kokugoba, ukugqwala, kanye nokuqhekeka kokugqwala kwengcindezi.Lezi zidingo zivame ukutholakala ezimbonini zasolwandle, zamakhemikhali, ne-petroleum.
Uma kudingeka i-post-weld annealing, le nsimbi yokushisela izodinga izinga lokushisa eliphakeme lokushisela kunalelo elidingwa i-duplex base metal.

INQUBO
Akukho ukushisa kwangaphambili.Izinga lokushisa eliphezulu lokungena elingu-300°F.
Ukufakwa kwe-annealing kungadingeka ukuze kuzuzwe ubulukhuni obufanayo kuma-weldments amaningi.
Okokufaka kokushisa kufanele kukhawulelwe ku-5-40 KJ/IN.

ICHEMISTRY EYEVAMILE

C Cr Ni Mo Mn Si P S N Cu
0.02 25.3 9.8 3.37 0.80 0.70 0.03 0.015 0.14 1.87

IZAKHIWO ZEMITHETHO EZIJWAYELEKILE

UBUNZIMA 25 RC as welded 35 RC umsebenzi onzima
AMANDLA OKUQHUBEKA 110,000 PSI Min.
ELONGATION 15% Amaminithi.

IMIPHAKATHI YOKUSHISA

SIZE I-VOLTAGE AMPERAGE IGAS
.045” 25-30 130-220 75% Ar / 25% CO2 noma 100% CO2

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besizibandakanya ekukhiqizeni ama-electrode wokushiselaizinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ihlanganisa ama-electrode ensimbi engagqwali, ama-electrode welding steel, i-low alloy welding electrode, ama-electrode welding angaphezulu, ama-electrode welding we-nickel & cobalt alloy, izintambo zokushisela zensimbi emnene & ne-alloy ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe igesi eziguquguqukayo, izintambo zokushisela i-aluminium, i-arc welding engaphansi kwamanzi.izintambo, izintambo zokushisela i-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode ama-tungsten, ama-electrode okugobhoza ikhabhoni, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.


  • Okwedlule:
  • Olandelayo: