I-electrode yokushisela yensimbi engagqwali ye-E308-16

Incazelo emfushane:

I-Electrode Yokushisela Yensimbi EngagqwaliI-E308-16 iyi-electrode yokushisela yohlobo lwe-titanium yomugqa wensimbi engagqwali enekhabhoni ephansi kakhulu.


  • :
  • Imininingwane Yomkhiqizo

    Amathegi Omkhiqizo

    I-AWS:SFA 5.4 E308-16 I-Electrode Yokushisela Yensimbi Engagqwali

    I-E308-16 uhlobo lwe-titanium oluyimigqai-electrode yokushiselayensimbi engagqwali enekhabhoni ephansi kakhulu.

    Ukuhlukaniswa:

    I-AWS A5.4 / ASME SFA5.4 E308-16

    I-JIS Z3221 D308-16

    Incazelo:

    I-Electrode Yokushisela Yensimbi Engagqwali E308-16 uhlobo lwe-titanium yomugqai-electrode yokushiselangensimbi engagqwali enekhabhoni ephansi kakhulu. Insimbi yokushisela inezakhiwo ezinhle kakhulu zomshini futhi ikhombisa ukumelana okuhle nokugqwala kwe-intergranular ngenxa yokuthi okuqukethwe yikhabhoni kuyo kungu-≤. 0.04% b. Ingasetshenziswa kuzo zonke izindawo zokushisela ngokusebenza okuhle kakhulu: i-arc ezinzile, ama-spatter amancane, ukubukeka okuhle kwe-weld. Futhi i-electrode yokushisela ikhombisa ukumelana okuhle nokushisa, akulula ukuphenduka ibe bomvu futhi i-gas porosity ayikhiqizwa.

    Isicelo:

    Ukushisela kwensimbi engu-18% Cr-8% Ni.

    Ifanele izakhiwo zokushisela ezenziwe ngensimbi engagqwali ye-022Cr-19Ni10 ephansi kakhulu, njengefayibha yokwenziwa, umanyolo,

    imishini ye-petrochemical, njll.

     

    Ukwakheka Kwamakhemikhali Kwensimbi Egciniwe (E308L-16) (%)

    Into C Mn Si Cr Ni S P Cu Mo
    inani elijwayelekile ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
    Inani lesibonelo 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

    Izakhiwo Zemishini Zensimbi Egciniwe (%)

    Ukusebenza kokulwa nokugqwala kanye nokwakheka kwe-ferrite kufanele kunqunywe phakathi komthengi nomthengisi.

    Into Amandla Okudonsa (MPa) Ukwelulwa (%)
    inani elijwayelekile ≥550 ≥25
    Inani lesibonelo 601 41

    Izicelo

    Ingasetshenziswa ukushisela uhlobo olufanayo lwezakhiwo zensimbi engagqwali ezimelana nokushisa ezisebenza ekushiseni okuphezulu, ingasetshenziswa futhi ukushisela insimbi enkulu ye-chrome e-sclerosing (njenge-Cr15Mo, i-Cr9Mo, i-Cr13, i-Cr28) kanye nensimbi engafani.

    Ububanzi(mm)

    2.0

    2.5

    3.2

    4.0

    5.0

    Umshini Wokushisela (A)

    25-50

    50-80

    80-110

    110-160

    160-200

    Yamanje: AC noma DC+

    Amanothi Ngokusetshenziswa:

    1. Gcina i-arc imfushane ngangokunokwenzeka.

    2. Susa ukungcola okufana namafutha nothuli emseleni.

    3. Yomisa ama-electrode ku-350 (662) imizuzu engama-60 ngaphambi kokusebenzisa

     