Induku Yokushisela Yensimbi Engagqwali ye-E308L-17

Incazelo emfushane:

I-E308L-17 Yensimbi Engagqwali Yokushisela I-Electrode (I-C Ephansi, 18%Cr- 8%Ni)


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-E308L-17 Yensimbi Engagqwali Yokushisela I-Electrode (I-C Ephansi, 18%Cr- 8%Ni)

Ukuhlukaniswa ngezigaba

EN IS03581-A:2016: E 19 9 L R 12

I-EN IS03581-B:2016: ES308L-17

I-AWS A5.4-2014: E308L-17

I-JISZ 3221-2013: ES308L-17

Incazelo

-Isimbozo siwuhlobo lwe-lime titania lokushisela insimbi engagqwali engu-18%Cr-8%Ni. (AISI 301, 302, 304, 308)

-Ukusebenza kahle kakhulu kokushisela ngenxa yesilinganiso esiphezulu sokufakwa.

- Susa amanzi, ukugqwala, uwoyela nazo zonke izinto ezingaphandle emseleni ngaphambi kokushisela.

-Ukusetshenziswa okuhle ngezinhlelo zokusebenza zamanje eziqondile.

-Ukushisa kusengaphambili akudingekile ngokuvamile.

-Hlanza kabusha i-electrode ku-250~350°C imizuzu engama-30~60 ngaphambi kokusebenzisa.

Ukwakheka Kwamakhemikhali Insimbi Egciniwe (%)
C Mn Si Cr Ni S P Mo Cu Fn
0.03 0.65 0.73 18.95 9.82 0.012 0.028 0.21 0.30 6.4

 

Osayizi kanye Nokunconywa Kwamanje (i-AC noma i-DC)
Ububanzi benduku yokushisela
(mm)
2.5 3.2 4.0 5.0
ukushisela okwamanje
(A)
55-80 90-130 110-150 140-180

Izici Zokusetshenziswa:

I-arc eqinile kakhulu.

Ukususwa okuhle kakhulu kwe-slag.

Ukungena akujulile.

Ukumelana okuhle nokushisa nokugqwala.

Ukumelana okuhle kakhulu nokuqhekeka.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesineminyaka engu-22 sisebenza ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon nezinye izesekeli zokushisela kanye nezinto ezisetshenziswayo..


  • Okwedlule:
  • Olandelayo: