I-E70C-6M Carbon Steel Flux Cored Arc Welding Electrodes Flux Core Welding Wire

Incazelo emfushane:

Intambo yokushisela ene-metal cored ye-E70C-6M ihlanganisa ukusebenza kahle kwezintambo eziqinile (GMAW) namazinga aphezulu okukhiqiza izintambo ezine-flux-cored (FCAW) - amazinga aphansi okukhiqiza intuthu, ukusebenza kahle okuphezulu, akukho slag yokuhlanza noma ukususa - nazo zonke izinzuzo izintambo ezine-cored ezinazo ngaphezu kwezintambo eziqinile - akukho "i-cold lap" noma ukuntuleka kokuhlanganiswa kwe-sidewall, impumelelo yokufafaza okumsulwa ene-argon/ibhalansi ye-carbon dioxide engu-75-80%, isivinini sokuhamba esisheshayo sosayizi we-fillet onikeziwe.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Intambo yokushisela ene-metal-core ye-E70C-6M ihlanganisa ukusebenza kahle kwezintambo eziqinile (GMAW) ngezilinganiso eziphezulu zokukhiqiza zezintambo ezihlanganisiwe (FCAW) - amazinga aphansi okukhiqiza intuthu, ukusebenza kahle okuphezulu, akukho slag yokuhlanza noma ukususa - nazo zonke izinzuzo izintambo ezihlanganisiwe ezinazo ngaphezu kwezintambo eziqinile - akukho "i-cold lap" noma ukuntuleka kokuhlanganiswa kwe-sidewall, impumelelo yokufafaza okumsulwa ene-75-80% argon/balance carbon dioxide, isivinini sokuhamba esisheshayo sosayizi we-fillet onikeziwe. I-E70C-6M ifaneleka kahle ekusetshenzisweni lapho amazinga aphezulu e-manganese ne-silicon edingeka khona, njengalapho kukhona isikali esindayo se-mill noma ukungcola okuncane, noma lapho kudingeka ukumanzisa okungcono kwe-weld bead. Lo mkhiqizo uhamba phambili ekushiseni okujwayelekile, kodwa ungcono ngokulinganayo ezimweni ezifunwa kakhulu njengasekukhiqizweni kwensimbi esindayo, umsebenzi wesakhiwo, ukushisela amapayipi kanye nokushisela ama-heater amanzi ashisayo.

Ikilasi le-AWS: E70C-6M Isitifiketi: AWS A5.18/A5.18M: 2005
Ingxubevange: E70C-6M I-ASME SFA A5.18

 

Indawo Yokushisela: F, H, V, OH .035-1/16”
F, H 5/64”-1/8”
Okwamanje:
I-DCEP

 

Amandla Okudonsa, kpsi: 70 100% CO2
Amandla Okukhiqiza, kpsi: 58 100% CO2
Ukwandiswa ngo-2”%: 22 100% CO2

I-Chemistry ejwayelekile yezintambo ngokwe-AWS A5.18 (amanani alodwa aphezulu)

C Mn Si S P Ni Cr Mo V Cu  
0.12 1.75 0.90 0.03 0.03 0.50 0.20 0.30 0.08 0.50  
Amapharamitha Okushisela Ajwayelekile
Ububanzi Inqubo I-Volt Ama-Amps Igesi Yokuvikela
in (mm)
.035 (0.9) I-GMAW 24-35 160-250 75-95% Ar/ibhalansi Co2, 35-50cfh
.045 (1.2) I-GMAW 37-33 180-330 75-95% Ar/ibhalansi Co2, 35-50cfh
.052 (1.3) I-GMAW 25-35 220-460 75-95% Ar/ibhalansi Co2, 35-50cfh
1/16 (1.6) I-GMAW 26-37 240-520 75-95% Ar/ibhalansi Co2, 35-50cfh
5/64 (2) I-GMAW 27-36 240-550 75-95% Ar/ibhalansi Co2, 35-50cfh
3/32 (2.4) I-GMAW 28-36 350-550 75-95% Ar/ibhalansi Co2, 35-50cfh
7/64 (2.78) I-GMAW 27-34 400-600 75-95% Ar/ibhalansi Co2, 35-50cfh
1/8 (3.2) I-GMAW 26-32 95-145 75-95% Ar/ibhalansi Co2, 35-50cfh

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besilokhu sihilelekile ekukhiqizeni ama-electrode okushisela,izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.


  • Okwedlule:
  • Olandelayo: