I-ENiFe-CI Nickel Alloy Welding Wire, FN 55 Nickel Tig Wire Ferro-nickel Solid Wire

Incazelo emfushane:

Intambo eqinile ye-Ferro-nickel esetshenziselwa ukushisela insimbi ephonswe kanye nensimbi ethambile.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Nickel AlloyUcingo Lokushisela Intambo yeTigI-ENiFe-CI

Amazinga
I-EN ISO 1071 – SC NiFe-1
I-AWS A5.15 – E NiFe-CI

 

Izici kanye nezinhlelo zokusebenza

I-Ferro-i-nickelucingo oluqinile olusetshenziselwa ukushisela insimbi ephothiwe kanye nensimbi ethambile.

Ifanelekela ukuhlangana okuhlukile phakathi kwensimbi ephothiwe, insimbi ethambile, i-alloy ephansi kanye nensimbi engagqwali.

Kunconywa ukushisela ama-castings angcoliswe yi-sulphur ephezulu, i-phosphorus noma amafutha.

Ngokuvamile isetshenziselwa izinhlelo ezahlukene zokulungisa nokwakha, okuhlanganisa ukwakha kabusha imiphini, amasondo, izixhumanisi ezibalulekile phakathi kwensimbi nensimbi ephonswe njll.

Izinto Eziyisisekelo Ezijwayelekile

Insimbi empunga, ethambile, enamaqhubu*
* Uhlu olubonisayo, hhayi oluphelele

 

Ukwakheka Kwamakhemikhali %

C%

Mn%

I-Si%

P%

S%

   

ubuningi

ubuningi

ubuningi

ubuningi

ubuningi

   

2.00

0.80

0.20

0.03

0.03

   

   

I-Fe%

I-Ni%

I-Cu%

I-Al%

   

i-rem.

54.00

ubuningi

ubuningi

   

56.00

2.50

1.00

   

 

Izakhiwo Zemishini
Amandla Okudonsa 400 – 579 MPa  
Amandla Okukhiqiza -  
Ukwelulwa -  
Amandla Omthelela -  

Izakhiwo zemishini ziyalinganiselwa futhi zingahluka ngokuya ngokushisa, igesi yokuvikela, amapharamitha okushisela kanye nezinye izici.

 

Amagesi Okuvikela

I-TS EN ISO 14175 TIG: I1 (Argon)

 

Izikhundla Zokushisela

I-TS EN ISO 6947 PA, PB, PC, PD, PE, PF

 

Idatha Yokupakisha

Ububanzi

Ubude

Isisindo

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg