I-ER1100 A5.10 Intambo Yokushada Ye-Aluminium Izinduku Nama-Electrode

Incazelo emfushane:

I-ER1100 imelana kakhulu nokuhlaselwa ngamakhemikhali kanye nokuguquka kwesimo sezulu. Iyingxube ethambile kakhulu futhi etholakala kalula futhi isetshenziswa kakhulu emikhiqizweni ye-thin gauge kanye ne-foil.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Ama-electrode nezinduku ze-ER1100 A5.10, i-aluminium ne-aluminium ...

I-ER1100 imelana kakhulu nokuhlaselwa ngamakhemikhali kanye nokuguquguquka kwesimo sezulu. Iyingxube ethambile kakhulu eyenzeka kalula futhi isetshenziswa kakhulu emikhiqizweni ye-thin gauge kanye ne-foil. Inezici ezinhle zokumanzisa futhi isetshenziswa njengengxube yokugcwalisa ngezinjongo zokushisela. Isici esifiselekayo sengxube ukuqeda okukhanyayo okutholakala ngokufaka i-anodizing.

Izicelo Ezijwayelekile: ukushintshanisa ukushisa; imishini yokuphatha ukudla; ​​ama-rivets; ucingo lokubopha; ukwenza insimbi

Ikilasi le-AWS: ER1100 Isitifiketi: AWS A5.10/ A5.10M: 1999
Ingxubevange: ER1100 I-AWS/ASME SFA A5.10

 

Isikhundla Sokushisela:
F, V, OH, H
Okwamanje:
I-DCEP-GMAW
I-AC-GTAW

 

Izakhiwo Ezijwayelekile (njengoba zihlanganisiwe)

Ukuqhuba: 59% IACS (-12)
Amandla Okudonsa, kpsi: 13
Umbala: Okumpunga
Indawo Yokuncibilika 1215⁰F Ukuqina 1090⁰F Ubuningi 0.098 lbs/cu In.

I-Chemistry ejwayelekile ye-Wire ngokwe-AWS A5.10 (amanani alodwa aphezulu)

I-Si + Fe Cu Mn Zn Okunye Al  
0.95 0.05-0.20 0.05 0.10 0.15 99.0 min  
Amapharamitha Okushisela Ajwayelekile
Ububanzi Inqubo I-Volt Ama-Amps Igesi
in (mm)
.030 (.8) I-GMAW 15-24 60-175 I-Argon (cfh)
.035 (.9) I-GMAW 15-27 70-185 I-Argon (cfh)
3/64” (1.2) I-GMAW 20-29 125-260 I-Argon (cfh)
1/16” (1.6) I-GMAW 24-30 170-300 I-Argon (cfh)
3/32” (2.4) I-GMAW 26-31 275-400 I-Argon (cfh)
Ububanzi Inqubo I-Volt Ama-Amps Igesi
in (mm)
1/16” (1.6) I-GTAW 15 60-80 I-Argon (cfh)
3/32” (2.4) I-GTAW 15 125-160 I-Argon (cfh)
1/8” (3.2) I-GTAW 15 190-220 I-Argon (cfh)
5/32” (4.0) I-GTAW 15 200-300 I-Argon (cfh)
3/16” (4.8) I-GTAW 15-20 330-380 I-Argon (cfh)

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 


  • Okwedlule:
  • Olandelayo: