Incazelo emfushane:

I-ER5356 iyingxubevange yohlobo lwe-aluminiyamu yohlobo olujwayelekile oluvame ukukhethwa ngenxa yamandla ayo okugunda aphakeme uma kuqhathaniswa.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-ER5356 iyingxubevange yohlobo lwe-aluminiyamu yohlobo olujwayelekile oluvame ukukhethwa ngenxa yamandla ayo okugunda aphakeme uma kuqhathaniswa.Ngaphezu kwalokho, iphinde inikeze ukumelana nokugqwala okuhle kakhulu lapho kuvezwe emanzini anosawoti.I-ER5356 kufanele icatshangelwe ukushisela uchungechunge lwezinsimbi ze-aluminium 5000.

Izicelo Ezijwayelekile: i-welding filler wire

I-AWS Ikilasi: ER5356 Isitifiketi: AWS A5.10/ A5.10M:1999
Ingxubevange: ER5356 I-AWS/ASME SFA A5.10
Isikhundla sokushisela:
F, V, OH, H
Okwamanje:
I-DCEP-GMAW
I-AC-GTAW
Izakhiwo Ezijwayelekile (njengoba zishiselwe)
I-Conductivity: 29% IACS (-0)/27% IACS (-H18)
Amandla Okuqina, kpsi: 38
Umbala: Emhlophe
I-Melting Point 1175⁰F Ukuqinisa 1060⁰F Ukuminyana 0.096 lbs/cu In.
I-Typical Wire Chemistry njenge-AWS A5.10 ngayinye (amanani angawodwa aphezulu)
Si Fe Cu Mn Mg Cr Zn Ti Okunye AL
0.25 0.40 0.10 0.50-1.0 4.7-5.5 0.05-0.20 0.25 0.05-0.20 0.15 Okusele
Amapharamitha we-Welding ajwayelekile
Ububanzi Inqubo I-Volt Ama-Amps IGAS
in (mm)
.030 (.8) I-GMAW 15-24 60-175 I-Argon (cfh)
.035 (.9) I-GMAW 15-27 70-185 I-Argon (cfh)
3/64” (1.2) I-GMAW 20-29 125-260 I-Argon (cfh)
1/16” (1.6) I-GMAW 24-30 170-300 I-Argon (cfh)
3/32” (2.4) I-GMAW 26-31 275-400 I-Argon (cfh)
Ububanzi Inqubo I-Volt Ama-Amps IGAS
in (mm)
1/16” (1.6) I-GTAW 15 60-80 I-Argon (cfh)
3/32” (2.4) I-GTAW 15 125-160 I-Argon (cfh)
1/8” (3.2) I-GTAW 15 190-220 I-Argon (cfh)
5/32” (4.0) I-GTAW 15 200-300 I-Argon (cfh)
3/16” (4.8) I-GTAW 15-20 330-380 I-Argon (cfh)

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesineminyaka engaphezu kwengu-20 sisebenza ekwenzeni ama-welding electrode, izinduku zokushisela, nezinto ezisetshenziswayo zokushisela.

Imikhiqizo yethu eyinhloko ihlanganisa ama-electrode ensimbi engagqwali, ama-electrode welding steel, i-low alloy welding electrode, ama-electrode welding angaphezulu, ama-electrode welding we-nickel & cobalt alloy, izintambo zokushisela zensimbi emnene & ne-alloy ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe igesi eziguquguqukayo, izintambo zokushisela i-aluminium, i-arc welding engaphansi kwamanzi.izintambo, izintambo zokushisela i-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode ama-tungsten, ama-electrode okugobhoza ikhabhoni, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 


  • Okwedlule:
  • Olandelayo: