Izinduku Zokushisela Zensimbi Yekhabhoni ze-ER70S-2, Izinsimbi Zokugcwalisa Zentambo Yokushisela Evikelwe Yi-Arc Yegesi, Umhlinzeki Ongcono Kakhulu Wokushisela

Incazelo emfushane:

I-ER70S2 iyintambo ye-MIG ne-TiG esezingeni eliphezulu yokushisela kuzo zonke izinhlobo zezinsimbi ezithambile neze-carbon, ikhiqiza ukushisela kwekhwalithi ephezulu okunezimbobo ezincane.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-ER70S2 iyintambo ye-MIG ne-TiG esezingeni eliphezulu yokushisela kuzo zonke izinhlobo zezinsimbi ezithambile neze-carbon, ikhiqiza ukushisela kwekhwalithi ephezulu okunezimbobo ezincane. Iyintambo ephindwe kathathu e-deoxidized (i-Zirconium, i-Titanium, ne-Aluminium) okwenza kube ukukhetha okuhle kakhulu kokushisela phezu kokugqwala kanye nesilinganiso sokugaya. Akukho ukugeleza okudingekayo ngalo mkhiqizo.

Izicelo Ezijwayelekile:

amapayipi kanye nemishini yokubhoboza ogwini lolwandle, umsebenzi wensimbi yokwakha

Isikhundla Sokushisela: F, V, OH, H Okwamanje: DCEP
Amandla Okudonsa, kpsi: 70
Amandla Okukhiqiza, kpsi: 58
Ukwandiswa ngo-2”%: 22

I-Charpy V-Notch ejwayelekile: 35 ft.-lb. Ku--20 deg F

I-Chemistry ejwayelekile yezintambo ngokwe-AWS A5.18 (amanani alodwa aphezulu)

C Mn Si P S Ni Cr Mo V Cu Ti Zr Al
0.07 0.90-1.40 0.40-0.70 0.025 0.035 0.15 0.15 0.15 0.03 0.50 0.05-0.15 0.02-0.12 0.05-0.15
Amapharamitha Okushisela Ajwayelekile
Ububanzi Inqubo I-Volt Ama-Amps Igesi Yokuvikela
in (mm)
.035 (0.9) I-GMAW 28-32 165-200 Ukudluliselwa Kwesifutho 98% Argon+2% Oxygen noma 75% Argon+25% CO2
.045 (1.2) I-GMAW 30-34 180-220 Ukudluliselwa Kwesifutho 98% Argon+2% Oxygen noma 75% Argon+25% CO2
1/16 (1.6) I-GMAW 30-34 230-260 Ukudluliselwa Kwesifutho 98% Argon+2% Oxygen noma 75% Argon+25% CO2
.035 (0.9) I-GMAW 22-25 100-140 Ukudluliselwa Kwesekhethi Esifushane 100% CO2 noma 75% Argon +25% CO2
.045 (1.14) I-GMAW 23-26 120-150 Ukudluliselwa Kwesekhethi Esifushane 100% CO2 noma 75% Argon +25% CO
1/16 (1.6) I-GMAW 23-26 160-200 Ukudluliselwa Kwesekhethi Esifushane 100% CO2 noma 75% Argon +25% CO
.035 (0.9) I-GTAW 13-16 60-100 I-Argon engu-100%
.045 (1.14) I-GTAW 13-16 70-120 I-Argon engu-100%
1/16 (1.6) I-GTAW 12-15 100-125 I-Argon engu-100%
3/32 (2.4) I-GTAW 15-20 125-175 I-Argon engu-100%
1/8 (3.2) I-GTAW 15-20 175-250 I-Argon engu-100%