I-Tig kanye ne-Mig Wire A5.28 ER80S-D2, Izinsimbi Zokugcwalisa Insimbi Ezingenamsoco Eziphansi Zokushisela I-Arc Evikelwe Ngegesi

Incazelo emfushane:

I-ER80S-D2 iyintambo eqinile yensimbi ethambile esetshenziswa ezimweni lapho ukugoba kuyinkinga noma lapho kufanele ulwe nokuqukethwe kwe-sulfur ephezulu noma ikhabhoni ensimbini yakho eyisisekelo.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-A5.28 ER80S-D2, Izinsimbi Zokugcwalisa Insimbi Ezingenamsoco Eziphansi Zokushisela I-Arc Evikelwe Ngegesi

I-ER80S-D2 iyintambo eqinile yensimbi ethambile esetshenziswa ezimweni lapho ukubhoboka kuyinkinga noma lapho kufanele ulwe nokuqukethwe kwe-sulfur ephezulu noma ikhabhoni ensimbini yakho eyisisekelo. Iqukethe amazinga aphezulu e-manganese ne-silicon ukuhlinzeka ngokumanzisa okuhle kanye nokubekezelela ukugqwala okuhle kanye nokukala.

Izicelo Ezijwayelekile: Izicelo zekhwalithi ye-x-ray, ama-weld anamandla aphezulu, ama-steam boilers, amathangi okucindezela, amapayipi egesi, ukushintshana kokushisa, imboni ye-petrochemical

Ikilasi le-AWS: ER80S-D2 Isitifiketi: AWS A5.28/A5.28M:2005
Ingxubevange: ER80S-D2 I-AWS/ASME SFA A5.28

 

Isikhundla Sokushisela: F, V, OH, H Okwamanje:
I-GMAW-DCEP

 

Amandla Okudonsa, kpsi: imizuzu engama-80
Amandla Okukhiqiza, kpsi: imizuzu engama-68
Ukwandiswa %: imizuzu eyi-17

I-Chemistry ejwayelekile ye-Wire ngokwe-AWS A5.28 (amanani alodwa aphezulu)

C Mn Si P S Ni Mo Cu Okunye
0.07-0.12 1.60-2.10 0.50-0.80 0.025 0.025 0.15 0.40-0.60 0.50 0.50
Amapharamitha Okushisela Ajwayelekile
Ububanzi Inqubo I-Volt Ama-Amps Igesi Yokuvikela
in (mm)
.035 (0.9) I-GMAW 28-32 165-200 Ukudluliselwa kwesifutho 98% Argon/2% Oxygen
.045 (1.2) I-GMAW 30-34 180-220 Ukudluliselwa kwesifutho 98% Argon/2% Oxygen
1/16 (1.6) I-GMAW 30-34 230-260 Ukudluliselwa kwesifutho 98% Argon/2% Oxygen
.035 (0.9) I-GMAW 22-25 100-140 Ukudluliselwa Kwesekhethi Esifushane 90% Helium/ 75% Argon / 25% CO2
.045 (1.2) I-GMAW 23-26 120-150 Ukudluliselwa Kwesekhethi Esifushane 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) I-GMAW 23-26 160-200 Ukudluliselwa Kwesekhethi Esifushane 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) I-GTAW 12-15 100-125 I-Argon engu-100%
3/32 (2.4) I-GTAW 15-20 125-175 I-Argon engu-100%
1/8 (3.2) I-GTAW 15-20 175-250 I-Argon engu-100%

 