I-ERCuSn-A (i-Phos Bronze A) I-Copper ne-Copper Alloy Bare Rods kanye ne-Electrodes Tig ne-Mig Wire

Incazelo emfushane:

I-ERCuSn-A Phos Bronze A iyithusi le-zinc yethusi eliqukethe cishe ithini elingu-5% kanye ne-phosphorus efika ku-0.35% engezwe njenge-deoxidizer esetshenziselwa ukushisela ithusi nethusi.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-ERCuSn-A Phos Bronze A iyithusi le-zinc yethusi eliqukethe cishe ithini elingu-5% kanye ne-phosphorus efika ku-0.35% engezwe njenge-deoxidizer esetshenziselwa ukushisela ithusi nethusi.Ingase futhi isetshenziselwe ukushisela ithusi uma ukuba khona kwethini kunsimbi yokushisela kungenakuphikiswa.

Izicelo Ezijwayelekile: ukumbozwa kwensimbi;ukuhlanganiswa kwe-509-519 yochungechunge lwezinsimbi ze-tin-bronze base

I-AWS Ikilasi: ERCuSn-A Isitifiketi: AWS A5.7/A5.7M:2007
Ingxubevange: ERCuSn-A I-ASME SFA A5.7

 

Isikhundla sokushisela: Okwamanje:
AC-DCEP

 

Amandla Okuqina, kpsi: 35
Ukuqina kweBrinell 70-85

I-Typical Wire Chemistry njenge-AWS A5.7 ngayinye (amanani angawodwa aphezulu)

Cu kubandakanya u-Ag Al Pb P Sn Okunye
Okusele 0.01 0.02 0.10-0.35 4.0-6.0 0.50

 

Amapharamitha we-Welding ajwayelekile
Ububanzi Inqubo I-Volt Ama-Amps IGAS
in (mm)
1/16 (1.6) I-GTAW 70-120 70-150 I-ACHF isebenzisa 100% Argon noma Helium 2% Thoriated, Ceriated noma Lanthanum Tungsten Electrode
3/32 (2.4) I-GTAW 120-160 140-230 I-ACHF isebenzisa 100% Argon noma Helium 2% Thoriated, Ceriated noma Lanthanum Tungsten Electrode
1/8 (3.2) I-GTAW 170-230 225-320 I-ACHF isebenzisa 100% Argon noma Helium 2% Thoriated, Ceriated noma Lanthanum Tungsten Electrode
Amapharamitha we-Welding ajwayelekile
Ububanzi Inqubo I-Volt Ama-Amps IGAS
in (mm)
0.035 (1.6) I-GMAW 20-26 100-200 100% Argon noma 75% Argon, 25% Helium
0.045 (2.4) I-GMAW 22-28 100-250 100% Argon noma 75% Argon, 25% Helium
1/16 (3.2) I-GMAW 29-32 250-400 100% Argon noma 75% argon, 25% Helium
3/32 (3.2) I-GMAW 32-34 350-500 100% Argon noma 75% Argon, 25% Helium

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesineminyaka engaphezu kwengu-20 sisebenza ekwenzeni ama-welding electrode, izinduku zokushisela, nezinto ezisetshenziswayo zokushisela.

Imikhiqizo yethu eyinhloko ihlanganisa ama-electrode ensimbi engagqwali, ama-electrode welding steel, i-low alloy welding electrode, ama-electrode welding angaphezulu, ama-electrode welding we-nickel & cobalt alloy, izintambo zokushisela zensimbi emnene & ne-alloy ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe igesi eziguquguqukayo, izintambo zokushisela i-aluminium, i-arc welding engaphansi kwamanzi.izintambo, izintambo zokushisela i-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode ama-tungsten, ama-electrode okugobhoza ikhabhoni, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 

 

 