Intambo Yokushisela ye-ERNiFeCr-1 Nickel Alloy, Insimbi Yokugcwalisa Intambo ye-Nickel Tig

Incazelo emfushane:

I-Alloy 825 (ERNiFeCr-1) iyintambo ye-nickel-iron-chromium okwenza lokhu kube ukukhetha okufanele kwezinhlobo ezahlukene zezicelo ezinzima.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Nickel AlloyUcingo LokushiselaIntambo yeTigI-ERNiFeCr-1

Amazinga
I-EN ISO 18274 – Ni 8065 – NiFe30Cr21Mo3
I-AWS A5.14 – ER NiFeCr-1

 

Izici kanye nezinhlelo zokusebenza

I-Alloy 825 iyi-i-nickelucingo lwe-iron-chromium olwenza lokhu kube ukukhetha okufanele kwezinhlobo ezahlukene zezicelo ezinzima.

Lolu cingo lunikeza amazinga aphezulu okumelana nokugqwala kokubili ezindaweni ezinciphisa i-oxidation kanye nezinciphisayo.

Ilungele ukumbozwa kwe-overlay lapho kudingeka khona ukwakheka kwamakhemikhali okufanayo.

Ukushibilika okuhle kakhulu ngensimbi yokushibilika e-austenitic ngokugcwele enokumelana okuphezulu nokuqhekeka kokugqwala kokucindezeleka kuma-media aqukethe ama-ion e-chloride.

Ngokuvamile isetshenziswa embonini yokucubungula amakhemikhali, i-petrochemical, ukukhiqizwa kwephepha kanye nokukhiqizwa kwamandla njll.

 

Izinto Eziyisisekelo Ezijwayelekile

I-G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, ALLOY 825, N08028, UNS N08825 W.Nr: 1.4500, 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465, 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586*
* Uhlu olubonisayo, hhayi oluphelele

 

Ukwakheka Kwamakhemikhali %

C%

Mn%

I-Fe%

P%

S%

I-Si%

 

ubuningi

0.70

22.00

ubuningi

ubuningi

ubuningi

 

0.05

0.90

umzuzu

0.020

0.004

0.50

 

 

I-Cu%

I-Ni%

I-Al%

I-Ti%

I-Cr%

Inyanga%

 

2.30

43.00

ubuningi

1.00

22.00

3.00

 

3.00

46.00

0.20

1.20

23.50

3.50

 

 

Izakhiwo Zemishini
Amandla Okudonsa ≥550 MPa  
Amandla Okukhiqiza -  
Ukwelulwa -  
Amandla Omthelela -  

Izakhiwo zemishini ziyalinganiselwa futhi zingahluka ngokuya ngokushisa, igesi yokuvikela, amapharamitha okushisela kanye nezinye izici.

 

Amagesi Okuvikela

I-TS EN ISO 14175 TIG: I1 (Argon)

 

Izikhundla Zokushisela

I-TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Idatha Yokupakisha
Ububanzi Ubude Isisindo  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

 