Intambo Yokushisela Ene-Flux Cored, Ibanga: Intambo Yensimbi Engagqwali engu-A 5.22 E308L T1-1

Incazelo emfushane:

Ukushisela izinsimbi ze-Low Carbon 18-20% Cr/ 8-12% Ni ezinekhono elihle kakhulu lokushisela Ngenxa yokuba khona kwe-ferrite, insimbi yokushisela inamandla aphansi okushelela ekuqhekekeni. Izakhiwo zemishini zingcono kakhulu esimweni sokushisela futhi zinokumelana okungcono kokugqwala phakathi kwe-granular ngenxa yokuqukethwe okuphansi kwekhabhoni.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Flux Cored Ucingo Lokushisela, Ibanga: A 5.22 E308l T1-1

Ukucaciswa Komkhiqizo

Izinto Zocingo SS
Ubuningi Nge-Roll ngayinye 15 kg
Ukupakisha 15 kg ngephakethe ngalinye
Ibanga I-A 5.22 E308L T1-1
Uhlobo Lokupakisha I-spool ivalwe esikhwameni se-polythene bese i-shrink igoqwe ebhokisini elihlanganisiwe
Ubukhulu 1.2MM 1.6MM
Okwamanje 190-300A
Isandiso Sentambo 20-25mm (inamathela)
Usayizi Otholakalayo 2.00mm, 2.4mm
I-Polarity Intambo ye-DC enhle
Igesi Yokuvikela Igesi ye-CO2 enesilinganiso sokugeleza esingamalitha ayi-15-20 ngomzuzu
Izakhiwo Zomshini Wokushisela I-UTS=520N/mm2 Min; Ubude(%)=35% min
I-chemistry yensimbi ehlanganisiwe C= 0.035%,Mn=1.65%,P=0.02%,Si=0.50%,S=0.008%,Ni=9.50%,Cr=19.50%

Incazelo Yomkhiqizo
Intambo yensimbi engagqwali egeleza nge-cored ene-arc ezinzile nebushelelezi, enokuhlukaniswa okuhle kwe-slag

Izicelo:
Ukushisela izinsimbi ze-Low Carbon 18-20% Cr/ 8-12% Ni ezinekhono elihle kakhulu lokushisela Ngenxa yokuba khona kwe-ferrite, insimbi yokushisela inamandla aphansi okushelela ekuqhekekeni. Izakhiwo zemishini zingcono kakhulu esimweni sokushisela futhi zinokumelana okungcono kokugqwala phakathi kwe-granular ngenxa yokuqukethwe okuphansi kwekhabhoni.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besilokhu sihilelekile ekukhiqizeni ama-electrode okushisela,izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.