I-Low Alloy Steel Welding Electrode AWS E9016-D1

Incazelo emfushane:

I-J606 (AWS E9016-D1) i-electrode yensimbi ephansi ye-alloy enamandla ene-low-hydrogen potassium coating.Ingasetshenziselwa ukushisela yonke indawo nge-AC ne-DC.Ukuzinza kokusebenza kwe-AC welding kungaphansi kwalokho kwe-DC welding.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Electrode ephansi ye-Alloy Steel Welding

J606                                       

I-GB/T E6016-D1

I-AWS E9016-D1 

 

Incazelo: I-J606 iyi-electrode yensimbi ene-alloy ephansi ene-low-hydrogen potassium coating.Ingasetshenziselwa ukushisela yonke indawo nge-AC ne-DC.Ukuzinza kokusebenza kwe-AC welding kungaphansi kwalokho kwe-DC welding. 

Isicelo: Isetshenziselwa ukushisela i-medium carbon steel kanye ne-low-alloy high-strength steel izakhiwo zamandla ahambisanayo, njenge-Q420, njll.

 

Ukwakheka kwamakhemikhali ensimbi ye-weld(%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Izici zemishini ye-weld metal:

Into yokuhlola

Amandla aqinile

Mpa

Amandla esivuno

Mpa

Ukwelula

%

Inani lomthelela (J)

-30 ℃

Kuqinisekisiwe

≥590

≥490

≥15

≥27

Ihloliwe

620 ~ 680

≥500

20 ~ 28

≥27

 

Okuqukethwe kwe-hydrogen okusabalaliswa kwensimbi efakiwe: ≤4.0mL/100g (indlela ye-glycerin)

Ukuhlolwa kwe-X-ray: I grade

 

Okwamanje okunconyiwe:

(mm)

Ububanzi benduku

2.0

2.5

3.2

4.0

5.0

5.8

(A)

I-Welding Yamanje

40 ~ 70

70 ~ 90

90 ~ 120

140 ~ 180

180 ~ 220

210 ~ 260

 

Isaziso:

1. I-electrode kufanele ibhakwe ihora elingu-1 ku-350 ℃ ngaphambi kokusebenza kokushisela;

2. Kubalulekile ukuhlanza okugqwalile, isikali sikawoyela, amanzi, nokungcola ezingxenyeni zokushisela ngaphambi kokushisela;

3. Sebenzisa ukusebenza kwe-arc emfushane lapho ushisela.Ithrekhi ewumngcingo yokushisela ilungile;

4. Uma ingxenye yokushisela isiwugqinsi, kufanele ifudunyezwe ibe ngaphezu kuka-150°C futhi ipholiswe kancane ngemva kokushisela.

 




  • Okwedlule: