Izinduku zokushisela i-AWS A5.1 E6013 (J421)

Incazelo emfushane:

Izinduku zokushisela i-AWS A5.1 E6013 (J421) ifanele ukushiselwa kwesakhiwo sensimbi ye-carbon ephansi, ikakhulukazi ukushiselwa kwensimbi yepuleti elincanyana eline-weld encishisiwe enesaphulelo kanye nemfuneko yephasi yokushisela ebushelelezi.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

Izinduku zokushisela i-AWS A5.1 E6013 (J421) ifanele ukushiselwa kwesakhiwo sensimbi ye-carbon ephansi, ikakhulukazi ukushiselwa kwensimbi yepuleti elincanyana eline-weld encishisiwe enesaphulelo kanye nemfuneko yephasi yokushisela ebushelelezi.

Izigaba:

ISO 2560-A-E35 0 RA 12

I-AWS A5.1: E6013

I-GB/T 5117 E4313

Izici:

I-AWS A5.1 E6013 (J421) iwuhlobo lwe-electrode ye-rutile.Kungaba i-welding kokubili umthombo wamandla we-AC & DC futhi ingaba kuzo zonke izindawo.Inokusebenza okuhle kakhulu kwe-welding njenge-arc ezinzile, i-spatter encane, ukususwa kwe-slag okulula kanye nekhono lokubusa njll. I-electrode ye-Rutile-cellulosic enekhono elihle lokushisela kuzo zonke izikhundla ezihlanganisa phansi mpo.Ikhono elihle kakhulu lokuvala igebe kanye nekhono lokushaya i-arc.Okokufaka i-tack welding kanye ne-load fit ups.Inhloso ejwayelekile yezimboni nezohwebo, ukuhlanganisa nokushisela izitolo.

Qaphela:

Ngokuvamile, awudingi ukomisa kabusha i-electrode ngaphambi kokushisela.Uma ithinteka ngokuswakama, kufanele yomiswe kabusha ku-150℃-170℃ ihora elingu-0.5-1.

Isikhundla sokushisela:

PA, PB, PC, PD, PE, PF

I-AWS A5.1 E6013 ifanelekela izakhiwo zokushisela ezenziwe nge-carbon steel low, yenza kahle kakhulu ekushiseleni amapuleti ensimbi amancane nosayizi omncane futhi isebenza kahle kakhulu esimweni esidinga ukubukeka kobuhlalu obuhle nobuhlanzekile.

Ukwakhiwa Kwekhemikhali kwayo Yonke Insimbi Yensimbi: (%)

Ukwakheka Kwamakhemikhali

C

Mn

Si

S

P

Ni

Cr

Mo

V

Izimfuneko

≤0.10

0.32-0.55

≤0.30

≤0.030

≤0.035

≤0.30

≤0.20

≤0.30

≤0.08

Imiphumela Ejwayelekile

0.08

0.37

0.18

0.020

0.025

0.030

0.035

0.005

0.004

Izakhiwo Zemishini Yensimbi Ebekiwe

Into yokuhlola

Rm (N/mm2)

I-Rel (N/mm2)

A (%)

I-KV2(J) 0℃

Izimfuneko

440-560

≥355

≥22

≥47

Imiphumela Ejwayelekile

500

430

27

80

Ireferensi Yamanje (DC)

Ububanzi

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

I-Amperage

40 ~ 70

50 ~ 90

80 ~ 130

150 ~ 210

180 ~ 240