I-AWS E6010 I-Electrode Yensimbi Yokushisela eMild, Izinduku zokushisela ze-Carbon Steel, i-High Cellulose Welding Stick

Incazelo emfushane:

I-J425G (AWS E6010) iyi-electrode ephezulu ye-cellulose ehlanganiswe ne-sodium eqondile eya phansi.


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

I-Carbon Steel Welding Electrode 

J425G                                                       

I-GB/T E4310

I-AWS A5.1 E6010

Incazelo: I-J425G iyi-electrode ephezulu ye-cellulose ehlanganiswe ne-sodium eqondile eya phansi.Sebenzisa i-DCEP (i-electrode eqondile yamanje eqondile), elungele ukushisela okuya phansi okuma mpo yonke indawo komthungo oyindilinga endaweni yepayipi.Uma welding ungqimba olungezansi, kungenziwa ashiselwe ohlangothini olulodwa futhi yakhelwe nhlangothi zombili, futhi isivinini Welding kuyashesha.

Isicelo: Isetshenziselwa ukushisela i-seam ye-circumferential yamapayipi e-carbon steel ahlukahlukene.

 

Ukwakheka kwamakhemikhali ensimbi ye-weld(%):

C

Mn

Si

S

P

≤0.20

0.30~0.60

≤0.20

≤0.035

≤0.040

 

Izici zemishini ye-weld metal:

Into yokuhlola

Amandla aqinile

Mpa

Amandla esivuno

Mpa

Ukwelula

%

Inani lomthelela (J)

(-30℃)

Kuqinisekisiwe

≥420

≥330

22

≥27

 

Ukuhlolwa kwe-X-ray: II grade

 

Okwamanje okunconyiwe:

Ububanzi benduku

(mm)

2.5

3.2

4.0

5.0

Welding current

(A)

40 ~ 70

70 ~ 110

110 ~ 160

160 ~ 190

 

Isaziso:

1. Khipha induku yokushisela ngaphambi kokuyisebenzisa, futhi uyisebenzise kakhulu ngangokunokwenzeka ngemva kokuyiqaqa;

2. Ngokuvamile, asikho isidingo sokuyomisa futhi ngaphambi kokushisela, futhi kungomiswa ku-70 ~ 90 ° C ihora elingu-1 uma kunomswakama.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesineminyaka engaphezu kwengu-20 sisebenza ekwenzeni ama-welding electrode, izinduku zokushisela, nezinto ezisetshenziswayo zokushisela.

Imikhiqizo yethu eyinhloko ihlanganisa ama-electrode ensimbi engagqwali, ama-electrode welding steel, i-low alloy welding electrode, ama-electrode welding angaphezulu, ama-electrode welding we-nickel & cobalt alloy, izintambo zokushisela zensimbi emnene & ne-alloy ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe igesi eziguquguqukayo, izintambo zokushisela i-aluminium, i-arc welding engaphansi kwamanzi.izintambo, izintambo zokushisela i-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode ama-tungsten, ama-electrode okugobhoza ikhabhoni, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 