Intambo Yokushisela ye-Nickel Alloy ERNiCu-7 Nickel Tig Wire Filler Metal

Incazelo emfushane:

I-ERNiCu-7 iyi-alloy ye-nickel-copper eyenzelwe ukushisela i-Monel.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Nickel AlloyUcingo LokushiselaIntambo yeTigI-ERNiCu-7

Amazinga
EN ISO 18274 – Ni 4060 – NiCu30Mn3Ti
I-AWS A5.14 – ER NiCu-7

 

Izici kanye nezinhlelo zokusebenza

Ingxubevange ye-nickel-copper eyenzelwe ukushisela i-Monel.

Ukubukeka okuhle kobuhlalu kanye nokumelana okuhle kakhulu nokugqwala ezixazululweni zikasawoti.

Insimbi ehlanganisiwe inokumelana okuhle kakhulu nenani elikhulu lezinto ezibolayo.

Le alloy isetshenziselwa futhi ukumbozwa kwe-weld.

Ngokuvamile kusetshenziswa ekwakhiweni kolwandle, ikakhulukazi ogwini lolwandle, ama-heat exchanger, amapayipi, izitshalo zokususa usawoti emanzini, izimboni zamakhemikhali, ze-petrochemical kanye nobunjiniyela bamandla njll.

Izinto Eziyisisekelo Ezijwayelekile

Ama-alloy e-Monel angu-400 no-404*
* Uhlu olubonisayo, hhayi oluphelele

 

 

Ukwakheka Kwamakhemikhali %

C%

Mn%

I-Fe%

P%

S%

I-Si%

ubuningi

3.00

0.50

ubuningi

ubuningi

ubuningi

0.15

4.00

2.50

0.020

0.015

1.00

I-Cu%

I-Ni%

I-Co%

I-Ti%

I-Al%

I-Nb+Ta%

28.00

62.00

ubuningi

1.50

ubuningi

ubuningi

32.00

69.00

1.00

3.00

1.00

0.50

 

Izakhiwo Zemishini
Amandla Okudonsa ≥450 MPa
Amandla Okukhiqiza ≥180 MPa
Ukwelulwa ≥30%
Amandla Omthelela ≥80 J

Izakhiwo zemishini ziyalinganiselwa futhi zingahluka ngokuya ngokushisa, igesi yokuvikela, amapharamitha okushisela kanye nezinye izici.

 

Amagesi Okuvikela

I-TS EN ISO 14175 TIG: I1 (Argon)

 

Izikhundla Zokushisela

I-TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Idatha Yokupakisha

Ububanzi

Ubude

Isisindo

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

Isibopho: Nakuba kwenziwe yonke imizamo efanelekile ukuqinisekisa ukunemba kolwazi oluqukethwe, lolu lwazi lungashintsha ngaphandle kwesaziso futhi lungabhekwa njengolufanelekela isiqondiso esijwayelekile.


  • Okwedlule:
  • Olandelayo: