I-RBCuZn-A Naval Bronze (RBCuZn-A) I-Copper-Zinc brazing Ukushisela Insimbi yokugcwalisa ucingo

Incazelo emfushane:

I-ERCuSn-A I-Phos Bronze A iyithusi eliyi-zinc eliqukethe cishe i-tin engu-5% kanye ne-phosphorus efinyelela ku-0.35% engeziwe njenge-deoxidizer esetshenziselwa ukushisela ithusi nethusi.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-RBCuZn-A Naval Bronze (RBCuZn-A) iyinsimbi yokugcwalisa i-copper-zinc brazing equkethe inani elincane le-tin ukuthuthukisa amandla kanye nokumelana nokugqwala endaweni yokushisela. Kuyisinqumo esihle uma izakhiwo zamandla aphezulu ze-bronze ephansi yokufutha zingadingeki. I-borax-boric acid flux ngokuvamile iyadingeka lapho kushiswa ngalo mkhiqizo.

Ikilasi le-AWS: RBCuZn-A Isitifiketi: AWS A5.8/A5.8M: 2011
Ingxubevange: RBCuZn-A I-ASME SFA A5.8

 

Isikhundla Sokubhinca: H, V Ububanzi Bokubhinca:
1330-1550⁰F

 

Amandla Okudonsa, kpsi: 50
Ukwelulwa %, ubuncane: 30

 

Indawo Yokuncibilika 1650⁰F Ukuqina 1610⁰F Ukuqina kukaBrinell 70-90

I-Chemistry ejwayelekile yezintambo ngokwe-AWS A5.8 (amanani alodwa aphezulu)

Cu Zn Sn Pb Al Okunye
57.0-61.0 I-Rem 0.25-1.00 0.05 0.01 0.50

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 

 

 


  • Okwedlule:
  • Olandelayo: