Intambo Yokushisela Yensimbi ye-RBCuZn-B (Nickel Bronze)

Incazelo emfushane:

Insimbi yokugcwalisa i-brazing ye-RBCuZn-B Nickel Bronze (RBCuZn-B) ifana nethusi lolwandle kodwa iqukethe i-manganese nensimbi okwandisa ubulukhuni namandla e-weld deposit.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Insimbi yokugcwalisa i-brazing ye-RBCuZn-B Nickel Bronze (RBCuZn-B) ifana nethusi lolwandle kodwa iqukethe i-manganese nensimbi okwandisa ubulukhuni namandla ediphozithi yokushisela. Iphinde iqukethe i-nickel eqinisekisa ukusatshalaliswa okufanayo kwensimbi ediphozithini. Ilangabi elingathathi hlangothi noma elikhipha i-oxidizing kancane kanye ne-boric acid/boric type flux kufanele isetshenziswe.

Ikilasi le-AWS: RBCuZn-B Isitifiketi: AWS A5.8/A5.8M: 2011
Ingxubevange: RBCuZn-B I-ASME SFA A5.8

 

Isikhundla Sokubhinca: H, V Ububanzi Bokubhinca:
1620-1800⁰F

 

Amandla Okudonsa, kpsi: 60-78
Ukwelulwa %, ubuncane: 25

 

Indawo Yokuncibilika 1620⁰F Ukuqina 1590⁰F Ukuqina kukaBrinell 80-110

I-Chemistry ejwayelekile yezintambo ngokwe-AWS A5.8 (amanani alodwa aphezulu)

Cu Zn Sn Fe Mn Ni Pb Al Si Okunye
56.0-60.0 I-Rem 0.80-1.10 0.25-1.20 0.01-0.50 0.20-0.80 0.05 0.01 0.04-0.20 0.50

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Sesisebenze ekukhiqizeni ama-electrode okushisela, izinduku zokushisela, kanye nezinto ezisetshenziswayo zokushisela iminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 

 

 


  • Okwedlule:
  • Olandelayo: