I-Electrode Yokushisela I-AWS A5.4 E310Mo-16 Izinduku Zokushisela Zensimbi Engagqwali Ama-Electrode Anamathelayo

Incazelo emfushane:

I-A412 (AWS E310Mo-16) iyi-electrode yensimbi engagqwali ye-austenitic ehlanzekile ye-Cr26Ni21Mo2 ene-titanium calcium coating.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

Ukushisela Insimbi EngagqwaliI-electrode

A412                                 

I-GB/T E310Mo-16

I-AWS A5.4 E310Mo-16

Incazelo: I-A412 iyi-electrode yensimbi engagqwali ye-austenitic ehlanzekile ye-Cr26Ni21Mo2 ene-titanium calcium coating. Ingasetshenziswa kokubili i-AC ne-DC ngokusebenza okuhle kakhulu. Ngenxa yokuthi i-molybdenum yengezwa ensimbini efakiwe, ukumelana kwayo nomgodi, amandla okushisa kanye nokumelana nokuqhekeka konke kuthuthukisiwe uma kuqhathaniswa ne-A402 ne-A407.

Ukusetshenziswa: Isetshenziselwa ukushisela insimbi engagqwali engamelana nokushisa esebenza ngaphansi kwezimo zokushisa okuphezulu, futhi ingasetshenziswa futhi ekushiseleni izintambo zensimbi engagqwali, izinsimbi ezingafani, njll. Inokumelana okungcono kokuqhekeka lapho ishisela insimbi yekhabhoni kanye nensimbi ephansi ye-alloy enokuqina okuphezulu.

 

Ukwakheka kwamakhemikhali kwensimbi eshidiwe (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.030

 

 

Izakhiwo zemishini zensimbi yokushisela:

Into yokuhlola

Amandla okudonsa

I-Mpa

Ukwelulwa

%

Kuqinisekisiwe

≥550

≥25

 

I-current enconyiwe:

Ububanzi benduku

(mm)

2.0

2.5

3.2

4.0

5.0

Ukushisela Kwamanje

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

  1. I-electrode kumele ibhakwe ihora eli-1 cishe ku-150℃ ngaphambi kokusebenza kokushisela;
  2. Ngenxa yokuthi ukujula kokungena akujulile ngesikhathi sokushisela i-AC, ugesi we-DC kufanele usetshenziswe ngangokunokwenzeka ukuze kungene ukungena okujulile. Futhi ugesi akufanele ube mkhulu kakhulu ukuze kugwenywe ukubomvu kwenduku yokushisela.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besilokhu sihilelekile ekukhiqizenii-electrode yokushiselas, izinduku zokushisela, futhiizinto ezisetshenziswayo zokushiselaiminyaka engaphezu kwengu-20.

Imikhiqizo yethu eyinhloko ifaka phakathi ama-electrode okushisela ensimbi engagqwali, ama-electrode okushisela ensimbi yekhabhoni, ama-electrode okushisela aphansi, ama-electrode okushisela okungaphezulu, ama-electrode okushisela e-nickel & cobalt alloy, izintambo zokushisela zensimbi emincane & ephansi, izintambo zokushisela zensimbi engagqwali, izintambo ezivikelwe ngegesi, izintambo zokushisela ze-aluminium, ukushisela kwe-arc okungaphansi komhlaba. izintambo, izintambo zokushisela ze-nickel & cobalt alloy, izintambo zokushisela zethusi, izintambo zokushisela ze-TIG & MIG, ama-electrode e-tungsten, ama-electrode okugoqa i-carbon, nezinye izesekeli zokushisela nezinto ezisetshenziswayo.

 

 

 


  • Okwedlule:
  • Olandelayo: