Ama-electrode okuwelda asekelwe ku-Nickel asezingeni eliphezulu e-Tyue Brand AWS A5.11 ENiCu-7 Nickel, Izinduku zokuwelda ze-Nickel Alloy zokuwelda ze-Arc

Incazelo emfushane:


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

I-Electrode Yokushisela I-Nickel ne-Nickel Alloy

I-Ni207                                                     

I-GB/T ENi4060

I-AWS A5.11 ENiCu-7

Incazelo: I-Ni207 iyi-electrode ye-Monel alloy ene-hydrogen sodium coating ephansi. Isebenzisa i-DCEP (i-electrode yamanje eqondile) futhi isebenza kahle ekushiseni kanye nokumelana nokuqhekeka.

Isicelo: Sokushisela i-Monel noma izinsimbi ezingafani. Ingasetshenziswa futhi ekweluleni ungqimba lokushintshana lokushisela olumboziwe.

 

Ukwakheka kwamakhemikhali kwensimbi eshidiwe (%):

C

Mn

Fe

Si

Al

Ti

Cu

Nb

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤1.0

≤1.0

27.0 ~ 34.0

≤2.5

≥62.0

≤0.015

≤0.020

 

Izakhiwo zemishini zensimbi yokushisela:

Into yokuhlola

Amandla okudonsa

I-Mpa

Amandla okukhiqiza

I-Mpa

Ukwelulwa

%

Kuqinisekisiwe

≥480

≥200

≥27

 

I-current enconyiwe:

Ububanzi benduku

(mm)

3.2

4.0

Ukushisela okwamanje

(A)

90 ~ 110

110 ~ 150

 

Isaziso:

1. I-electrode kumele ibhakwe amahora ama-2 cishe ku-300℃ ngaphambi kokusebenza kokushisela;

2. Kubalulekile ukuhlanza okugqwalile, uwoyela, amanzi, kanye nokungcola ezingxenyeni zokushisela ngaphambi kokushisela. Zama ukusebenzisa i-arc emfushane ukushisela.

 