Ama-electrode e-ENiCrFe-3 e-Nickel

Incazelo emfushane:

I-electrode ifaka insimbi yokushisela engu-65Ni-20Cr-2Nb-1.5Mo.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo

IKHODI YE-ISO YE-EN: 14172:ENi6082

I-electrode ifaka insimbi yokushisela engu-65Ni-20Cr-2Nb-1.5Mo. Insimbi yokushisela esezingeni le-Radiographic enezakhiwo ezinhle kakhulu. Ifaneleka kahle kakhulu kuma-alloy okushisela anezinhlanganisela ezifanayo nawo, ukuze kufakwe insimbi ene-alloy ye-Nickel-Chromium-Iron lapho okuqukethwe okuphezulu kwe-Manganese kungeyona ingozi, ukuze kufakwe ohlangothini lwensimbi ye-Nickel Chromium-Iron kanye nezinhlanganisela zensimbi ezingafani. Ifanelekela ukumbozwa kwamapuleti okushisela. Kunconywa ngokukhethekile ukushisela izinsimbi ze-9% Ni zesevisi ye-cryogenic. Iphinde isetshenziswe ekushiseni ama-alloy e-Nickel-Chromium asetshenziselwa ukusetshenziswa kwezinga lokushisa eliphezulu njengezinto zokushisa zesithando namashubhu okulungisa.

UKWAKHIWA KWAMAKHEMIKHALI OKUJWAYELEKILE KWAYO YONKE INSIMBI EWELDWELD

Isici C Mn Si Cr Ni Fe Nb Cu Ti S P
Amaphesenti ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

IZIMPAHLA EZIJWAYELEKILE ZOMKHIQIZO ZONKE ZESIMBI ESIWELDWE

I-UTS YS Ukwelulwa Amandla Omthelela we-CVN (J) Ukwanda Kwaseceleni Amandla Okungena ku-
(i-MPa) (i-MPa) (L= 5d)% ku-Minus 196°C ku-minus 196°C (mm) 600°C amahora ayi-1000.
620 500 30 75 0.85 160 MPa

IDATHA ELIPHUTHUMAYO NELIPHAKILE: DC (+)

Usayizi (mm)

Ubude be-Dia x

5×350

4×350

3.15×350

2.5×350

Ibanga Lamanje (Ama-Amps)

150-180

120-150

80-110

60-70

Isisindo/Ibhokisi (kgs)

2.5

2.5

2.5

2.5

Ukuqapha

1. Qinisekisa ukuthi ama-electrode omile. Omisa kabusha ama-electrode ku-300-325°C ihora elilodwa.

2. Gcina i-arc emfushane, i-stringer bead futhi unciphise ukufakwa kokushisa.

3. Vumela ukushisela ukuthi kuphole kube ngaphansi kwama-degrees Celsius angu-50 ngaphambi kokufaka, bese ubeka ungqimba olulandelayo.